Dilatometry

DIL L76 Horizontal

Robust and affordable dilatometer for beginners

Description

To the point

The main area of application of the LINSEIS L76 Horizontal dilatometer series is the CTE measurement of ceramics, bricks, tiles, porcelain and building materials.
It is also widely used for quality control in the ceramics and  metal industry.

Thanks to the flexible interchangeable furnaces, the dilatometer covers a wide temperature range from RT to 1000°C, 1400°C and 1600°C.
The measuring systems are made of either quartz glass (up to 1100°C) or Al2O3 (up to 1600°C).

The sensor is an LVDT (Linear Variable Differential Transformer) with maximum precision and infinitely variable resolution.
In combination with our LINSEIS software, the dilatometer offers an excellent solution for CTE measurements in standard quality control.

The following physical properties can be measured with the device: CTE, linear thermal expansion, sintering temperature, phase transformations, softening points, decomposition temperatures and glass transition temperatures.

Unique features

Flexible interchangeable ovens for temperatures
from RT to 1000°C, 1400°C and 1600°C

Measuring systems made of
quartz glass (up to 1100°C)
or Al2O3 (up to 1600°C)

High-precision LVDT
sensor with infinitely
variable resolution

LINSEIS software package for excellent CTE measurements

Measurement of the following physical properties:
CTE, linear thermal expansion, Alpha Physical,
sintering temperature, phase transformations,
softening points, Decomposition temperatures,
glass transition temperatures

Questions? We're just a call away!

+1 (609) 223 2070

 

+49 (0) 9287/880 0

Our service is available Monday to
Thursday from 8 am to 4 pm
and Friday from 8 am to 12 pm.

We are here for you!

Specifications

MODEL

DIL L76 Horizontal*

Temperature range:RT – 1600 °C
LVDT
Delta L resolution:0.05 nm (digital)
Measuring range:+/- 2500 µm
Contact force:Manual adjustment up to 1 N
Optical encoder
Delta L resolution:1 nm
Measuring range:+/- 25000 µm
Automatic sample length detection:yes
Force modulation:no
Contact force:Manual adjustment up to 3 N
Multiple oven configuration:optional
Gas metering:Manual gas dosing or mass flow controller 1/3 or more gases
Contact force adjustment:–
Single and double dilatometer:–
Softening point detection:inclusive
Density determination:optional
L-DTA:optional
Rate-controlled sintering (RCS):optional
Thermal library (database):optional
Electrical thermostatting of the measuring head:inclusive
Low temperature measurement option:LN2
Vacuum-tight construction:–
Automatic evacuation system:–
OGS Oxygen Getter:–
*Specifications depend on the configurations

Accessories

  • Devices for sample preparation
  • Caliper for manual or online entry of the sample length
  • Various gas boxes: manual, semi-automatic and MFC controlled
  • Software option: rate-controlled sintering (RCS)
  • Various sample holders (size, material)

Software

Making values visible and comparable

The powerful LINSEIS thermal analysis software, which is based on Microsoft® Windows®, performs the most important function in the preparation, execution and evaluation of thermoanalytical experiments, in addition to the hardware used. With this software package, Linseis offers a comprehensive solution for programming all device-specific settings and control functions, as well as for data storage and evaluation. The package was developed by our in-house software specialists and application experts and has been tried and tested over many years.

Dilatometer functions

  • Glass transition and softening point determination
  • Automatic softening point switch-off, freely adjustable (system protection)
  • Display of absolute or relative shrinkage or expansion
  • Representation and calculation of technical / physical expansion coefficients
  • Rate-controlled sintering (software option)
  • Sintering process evaluation
  • Density determination
  • Automatic evaluation routines
  • System correction (temperature, zero curve, etc.)
  • Automatic zero point adjustment
  • Automatic punch contact pressure control

General functions

  • Real-time color display
  • Automatic and manual scaling
  • Display of the axes freely selectable (e.g. temperature (x-axis) against delta L (y-axis))
  • Mathematical calculations (e.g. first and second derivatives)
  • Saving complete evaluations
  • Multitasking function
  • Multi-user function
  • Zoom option for various curve sections
  • Any number of curves can be loaded on top of each other for comparison
  • Online Help Menu
  • Free labeling
  • EXCEL® and ASCII export of measurement data
  • Data smoothing
  • Zero curves are offset
  • Cursor function
  • Statistical curve evaluation (mean value curve with confidence interval)
  • Tabular printout of the data and expansion coefficients
  • Calculation of Alpha Phys, Alpha Tech, relative expansion L/L0
  • Curve arithmetic, addition, subtraction, multiplication

Applications

Application example: Glass sample, softening point

To measure a glass sample up to the softening point, a function can be set in the measuring program of the software to stop the heating when the softening point is reached.
The setting can be specified in µm or in % of the change in length.
If the set value of the measured ramp is exceeded due to the deformation caused by the softening of the material, the program switches to the next ramp, in which, for example, cooling is programmed or the heating is automatically switched off.
This allows the softening point to be measured automatically without manual intervention and at the same time protects the sample holder.

Well informed

Downloads

Everything at a glance

DIL L76 Horizontal

Robust and affordable dilatometer for beginners