Discover the Linseis blog: The latest insights and news from the world of measurement technology

LINSEIS Thermal Library

Identify materials and compare measurement data – reconcile thermal properties with reference values and proprietary measurements within a common database. Thermal and thermophysical measurements provide characteristic information about the behavior of materials. Melting temperatures, glass transitions, mass changes, or thermal transport properties can help characterize materials and identify differences between samples.

Polyurethane (PUR): Thermal properties, structure and applications

Hardly any other material combines as many properties in a single material system as polyurethane (PUR). From soft comfort foam in the furniture sector to tough elastomers in the automotive industry and high-strength protective coatings on metal and concrete – PUR adapts to the respective requirements because its molecular architecture can be specifically adjusted.

High Entropy Alloys (HEAs): Thermal analysis and thermophysical properties

High entropy alloys (HEAs) are now considered a key material class for high-performance applications in aerospace, power generation, turbines and reactor construction. Due to their complex, multi-component composition, they exhibit unique combinations of high strength, temperature and oxidation resistance – but at the same time they are extremely difficult to characterize.

FEP fluoropolymer: Thermal properties and industrial applications

FEP (Fluorinated Ethylene Propylene Copolymer) combines low friction, excellent electrical insulation and high optical clarity in one material – a combination that predestines it for dynamic applications in which media flow, movement and signal transmission must be reliably controlled. [1,2] The following text highlights the key structural and thermal properties of FEP and shows how these can be specifically characterized using thermal analysis methods – and corresponding solutions from Linseis.

EVA – ethylene vinyl acetate: material science, properties and applications

Ethylene-vinyl acetate (EVA) is a soft, semi-crystalline copolymer that impresses with its high flexibility, excellent damping properties and an exceptionally wide property window – precisely where classic polyethylenes, rigid thermoplastics or brittle elastomers reach their limits. By specifically adjusting the vinyl acetate content (VA) and the degree of cross-linking, EVA can be adjusted from transparent-soft to structurally stable and highly damping.

Thermal diffusivity in batteries: Influence on hot spots, thermal runaway and lifetime

Thermal diffusivity α describes how quickly a temperature disturbance spreads in a material. It is directly linked to the thermal conductivity via the relationship λ = α – ρ – cₚ and thus determines in lithium-ion cells whether locally generated heat – for example due to side reactions, current density nests or local overcharging – is dissipated quickly or builds up to a dangerous hot spot.

How to Measure Heat Capacity in Heat Transfer Fluids for Industrial Applications

Efficient process design in modern energy, chemical, and manufacturing industries increasingly relies on accurate transport and management of thermal energy by engineered fluids. Understanding and quantifying heat capacity—essentially answering “How much heat can be transported by a fluid?”

Differential thermal analysis (DTA) for the early detection of incompatibilities in polymer blends

In the development of modern polymer blends, the focus is on the targeted combination of different polymers in order to flexibly adapt material properties to application requirements. Incompatibilities or phase separation within these blends are one of the most common challenges, as they have a significant influence on the mechanical and thermal properties of the end product.

PFA (perfluoroalkoxy): High-performance fluoropolymer for critical process environments

Perfluoroalkoxy (PFA) is a high-performance fluoropolymer that combines almost universal chemical resistance with high thermal stability up to a continuous service temperature of 260 °C and thus offers extremely high process reliability in critical process environments.

Translucent and dimensionally stable – what can acrylic glass really do?

Polymethyl methacrylate (PMMA), also known as acrylic glass, is a versatile thermoplastic that is characterized by its high light transmission, dimensional stability and wide range of applications.

Laser dilatometry: Precise characterization of high-tech glasses through contactless thermal analysis

The development of modern glass materials places the highest demands on analytical methods. Particularly with sensitive high-tech glasses, thin films or microstructured glass ceramics, conventional measurement methods quickly reach their limits. Laser dilatometry has established itself as a pioneering technology that masters these challenges through contactless, high-precision measurements.

SAN plastics: Molecular orientation and crystallinity as key factors for mechanical stability

Styrene-acrylonitrile copolymer (SAN) is a versatile engineering plastic characterized by its unique material combination of 70-80% styrene and 20-30% acrylonitrile.

Laser Flash Analyzer: Modern thermal characterization of insulation materials in the construction industry

With increasing requirements for energy efficiency and sustainability, the precise characterization of thermal parameters of insulation materials is coming to the fore. Thermal conductivity (λ) is the key parameter for evaluating the insulation performance – both when new and over the entire life cycle of a building material.

Refractory Alloys: Production and application in extreme environments

Refractory alloys made from materials such as tungsten, molybdenum, niobium, tantalum, rhenium and vanadium play a key role in extreme applications in aerospace, nuclear technology, the high-temperature industry, medical technology and electronics

Thermal dilatation difference in bonded joints: Challenges and solutions for reliable bonded joints

In modern design concepts for automotive, aerospace and electronics, hybrid assemblies made of various lightweight materials such as aluminum, steel and carbon fiber reinforced plastics (CFRP) are increasingly being joined using adhesive bonding technology.

How Thermal Analysis Helps Predict and Reduce Microfiber Shedding from Textiles

In modern design concepts for automotive, aerospace and electronics, hybrid assemblies made of various lightweight materials such as aluminum, steel and carbon fiber reinforced plastics (CFRP) are increasingly being joined using adhesive bonding technology.

Thermomechanical analysis of metals – Reliable material characterization for steel and alloys

Companies in the steel and metal industry are faced with ever-increasing demands: Components must withstand high thermal loads, process windows must be precisely adhered to and targeted structural changes are often the key to improved material properties.

Advanced Kinetics and Process Analysis of Hydrogen Reduction of Iron Ore with Linseis TGA and STA Systems

The direct reduction of iron ore with hydrogen is central to the decarbonization of the steel industry. Hydrogen-based processes enable a significant reduction of CO₂ emissions compared to conventional reduction with carbon carriers.

Error detection through thermal analysis: How DSC improves functional prototypes in additive manufacturing

Additive manufacturing has established itself as a transformative technology in industrial production – particularly in the development of functional prototypes.

Polycarbonate: transparency and impact strength in technical applications

Polycarbonate (PC) is one of the most important engineering thermoplastics in modern materials technology. Its unique combination of high transparency, pronounced impact strength and outstanding thermal stability makes it an indispensable material in numerous industrial sectors.

Assessing Protein Stability: Analytical Strategies for Biomolecular Research

Understanding protein stability is fundamental for modern biochemistry, pharmaceutical research, and biotechnology.

Understanding Lipid Membrane Phase Transitions: The Role of Tm in Membrane Structure and Function

The study of phase transitions in lipid membranes is a cornerstone of modern biophysics, connecting the fundamentals of membrane science with real-world applications in drug delivery, pharmaceutical formulation, and materials engineering

Epoxy resins: Versatile high-performance materials for demanding applications

Epoxy resins are among the most versatile materials in modern materials science and form a central basis for sophisticated composite systems, high-performance adhesives and protective coatings

Polylactide (PLA) – from bioplastic to high-tech material with a sustainable future

Polylactide (PLA) is becoming increasingly important in the plastics industry and is considered a pioneering alternative to fossil-based plastics

Simultaneous thermal analysis for the characterization of active pharmaceutical ingredients

The pharmaceutical industry is faced with the continuous challenge of precisely evaluating the stability and thermal behavior of active ingredients

PPS plastic: The versatile high-performance thermoplastic for demanding industrial applications

Polyphenylene sulfide (PPS) is a partially aromatic, semi-crystalline polymer with a unique structure of benzene rings linked by sulfur atoms

PVDF (polyvinylidene fluoride): High-performance polymers for pharmaceutical and medical applications

Polyvinylidene fluoride (PVDF) has considerably expanded its technological applications thanks to its piezoelectric and pyroelectric properties as well as its mechanical, chemical and thermal resistance.

PEEK (polyetheretherketone) – The versatile high-performance plastic for extreme requirements

PEEK (polyether ether ketone) is one of the world’s most efficient high-performance plastics and impresses with its exceptional combination of mechanical, thermal and chemical resistance.

Thermomechanical analysis (TMA) to evaluate the sealing function in the engine compartment: aging and long-term behavior of elastomer seals

Elastomer sealing rubbers, such as those used in the engine compartment of motor vehicles and in aviation applications, are exposed to permanent thermomechanical loads.

Amorphous vs. semi-crystalline polymers: standard-compliant DSC measurement according to ISO 11357 & ASTM D3418

When it comes to characterizing polymers, differential dynamic calorimetry (DSC) is one of the most reliable methods.

Heat Flow Meter method: Effective quality control of the thermal conductivity of insulation boards made of mineral wool and PU foam

The Heat Flow Meter method (HFM) is based on the fundamental principle of heat transfer through a material. A sample is placed between two plates with defined temperatures – one with a warm surface and one with a cold surface

How do metal matrix reinforced composites enable the reusability of space components?

The return of a spacecraft to the Earth’s atmosphere is one of the most thermally demanding phases of a mission. During atmospheric re-entry, temperatures of over 1500 °C occur on the outside of the vehicle, caused by shock waves, frictional heat and plasma effects in the high atmosphere.

PTFE as a high-performance engineering material: properties, applications and future prospects

Polytetrafluoroethylene (PTFE), widely known under the trade name Teflon, has long since developed from its original application as a non-stick coating for cookware into one of the most important high-performance technical materials.

Thermodynamics meets biopharma – Why ITC is becoming increasingly relevant for laboratories

In preclinical drug development, everything revolves around understanding molecular interactions. Whether protein-ligand complexes, antibody-antigen binding or enzyme-inhibitor interactions – for the selection and optimization of biopharmaceutical active ingredients, it is not just whether a molecule binds, but how well, how strongly and why it binds.

Thermal properties of battery cells: The transient hot bridge as a key technology

The development of efficient and long-lasting batteries requires a detailed understanding of the thermophysical properties of cell components. Especially when characterizing lithium iron phosphate (LFP), nickel manganese cobalt oxide (NMC) and solid electrolytes, the precise measurement of thermal parameters is crucial in order to understand and control ageing mechanisms and efficiency losses during charging and discharging cycles.

Thermoplastic elastomers: flexible, moldable, sustainable

Thermoplastic elastomers (TPE) are revolutionizing modern materials science with their unique ability to combine the best properties of two polymer worlds. They combine the elastic flexibility of conventional rubber materials with the processing-friendly meltability of thermoplastics and have thus become a key technology in a wide range of technical and everyday applications.

TGA-based moisture and stability analysis of pharmaceutical gelatine capsules

Thermogravimetric analysis (TGA) is a key method in pharmaceutical and medical analysis for quantitatively monitoring the moisture behavior and stability of materials such as gelatine capsules under real storage conditions.

Heat storage with zeolites: Determination of adsorption isotherms using gravimetric sorption analysis

The use of zeolitic sorption materials for heat storage is a forward-looking approach in the energy sector, as they offer high storage energy densities and reversible charging/discharging behavior.

Identification of degradation products and monitoring of volatile additives in thermoplastics using EGA-FTIR

Evolved gas analysis in combination with Fourier transform infrared spectroscopy (EGA-FTIR) is an established method for analyzing the thermal stability and emissions of additives in thermoplastics such as polyethylene (PE), polypropylene (PP) and polyamide (PA).

Thin Film Analyzer (TFA): Universal platform for material innovations in the thin film sector

Material innovations in the field of organic semiconductors (P3HT, PEDOT:PSS), MoS₂ and graphene are core areas of modern research and development. Thin-film technologies open up a wide range of possible applications, from flexible electronics to energy-efficient sensors.

Tg determination with TMA: How thermoplastics react under mechanical load

The glass transition temperature (Tg) marks the transition of a thermoplastic from a brittle, glass-like state to a rubber-like behavior.

Thermal management as a key factor in lightweight construction

Lightweight construction is considered a strategic driver of innovation in numerous high-tech industries—from aerospace and electromobility to power electronics.

Influence of sintering atmospheres on green bodies – analysis by simultaneous thermal analysis

In the field of technical ceramics, the targeted influencing of material properties through controlled sintering atmospheres plays a central role.

Heat accumulators in the high-temperature range: materials with constant capacity over many cycles

In the course of industrial decarbonization, the efficient use of thermal energy is increasingly becoming the focus of energy technology.

TG/DTA in catalysis research: evaluating reaction behavior and stability

Catalysts are at the heart of many industrial processes, whether in chemical synthesis, exhaust gas treatment, or energy storage.

Thermal expansion

Thermal expansion is the change in a material’s dimensions due to temperature changes – a key factor in construction, engineering, and materials research.

Thermal conductivity measurement of nanomaterials

Nanomaterials are an integral part of modern key technologies. They are used in areas such as nanoelectronics, battery technology, medical technology and the energy industry.

Advancing Additive Manufacturing with Thermal Analysis

Additive manufacturing (AM), also known as 3D printing, is a process for building complex structures layer by layer.

Alloys and non-metallic materials

Alloys are metallic materials that play a central role in modern technology and industry. They are created by combining at least two elements, one of which is always a metal.

Efficient curing of epoxy resin: influencing factors and methods

Epoxy resin is a versatile and high-performance reactive resin that is used in numerous application areas such as the electrical industry, construction and the manufacture of fiber composites.

Thermal conductivity of porous carbon materials

Porous carbon materials, in particular carbon aerogels, are the focus of current research. These materials are characterized by an extremely low thermal conductivity, which is mainly due to their porous structure and low bulk density.

Glass Transition Temperature

The glass transition temperature Tg is a point on the temperature scale at which a polymer or glass changes into a rubbery, viscous state. However, this is not the same as the melting point.

Thermal Interface Materials – Overview and application

Thermal interface materials (TIMs) are used in the field of electronics to ensure efficient heat dissipation and prevent local temperature overloads.

Accurately measure Seebeck – importance in science and technology

The Seebeck effect enables the direct conversion of heat into electrical energy.

How does a pushrod dilatometer work?

A dilatometer is a measuring device for recording the thermal expansion of a material sample. The thermal expansion coefficient (CTE = Coefficient of Thermal Expansion) is calculated from the measurement results.

Crystallization and recrystallization of polymers

The properties of solids depend to a large extent on the arrangement of the particles (atoms and molecules) that make up the substances. If the arrangement is random, the substances are amorphous. In crystalline substances, the particles are arranged at regular intervals and in a fixed pattern.

Curing in thermal analysis

Materials that are processed in a liquid aggregate state generally require a certain amount of time to harden.

Specific heat capacity (Cp) with modulated DSC

The specific heat capacity (cp), often referred to as specific heat, is a fundamental thermophysical property of a material. It says something about the ability to store thermal energy.

Measurement of the specific heat capacity (cp) using the transient hot wire method

The specific heat capacity is a fundamental thermophysical property of materials and is useful for assessing materials and their areas of application. It can be determined using dynamic differential scanning calorimetry (DSC).

Characterization of photovoltaic materials by measuring the Hall voltage

Characterization of photovoltaic materials – The charge carrier mobility in semiconductor materials is an important parameter for their usability in solar cells.

How to correctly calibrate a Differential Scanning Calorimeter

Correct calibration of a DSC – Why is correct calibration so important? Thermoanalytical measurements are often used in quality assurance;

Melting point, crystallization, and glass transition in polymers

Melting point, crystallization and glass transition in polymers – The change in the aggregate state of a solid from solid to liquid is called melting.

Measuring Specific Heat Capacity (cp) using Laser Flash Analysis (LFA)

The specific heat capacity cp, thermal diffusivity a and thermal conductivity λ are important thermophysical material properties for characterizing the thermal conductivity of materials.

Phase transitions with dilatometer

A dilatometer can be used to determine phase transitions in materials, as a phase change is also accompanied by a change in the coefficient of thermal expansion (CTE) of the material.

Measurement of thermal stability

A plastic is thermally stable if it does not decompose under the influence of temperature. The opposite of thermostability is thermolability.

Real-time insight into the grain growth with the non-destructive NDT technology laser ultrasound

In cooperation with Linseis Messgeräte GmbH and RECENDT GmbH (Research Center for Non-Destructive Testing GmbH), a real-time grain size determination system based on a dilatometer system (DIL L78/RITA) and an adapted laser-ultrasonic system (LUS) was developed.

Phase transition of a substance: Melting

Melting describes the phase transition of a substance from a solid state to a liquid state.

What happens during Crystallization (Tc)?

Crystallization describes the transition of a substance into a crystalline state. This can occur from the gas phase, solid phase or liquid phase.

Investigations into hydrogen storage solutions

As the mass-specific energy density of hydrogen (33.3 kWh/kg) is one of the highest of all fuels, the use of hydrogen for mobility and as an energy storage medium was and is of great interest.

Specific heat capacity

The specific heat capacity indicates the ability of a substance to store heat. This material quantity corresponds to the amount of heat required to heat a certain amount of a substance by one Kelvin.

PCM – Phase Change Material

A second heat reservoir is the simple increase in temperature without a phase change. For such applications, the specific heat capacity of the storage material and its density should be high.

Thermal contact resistance

The thermal contact resistance characterizes the transfer of heat at the interface between two solids.

3D printing in ceramics

Ceramics are used in many areas of industry. As a rule, ceramics are first formed as green bodies from raw mass before this “green body” is then treated in a special way and fired (so-called sintering).

3D Printing Polymers

Injection molding, often also referred to as injection molding or injection molding process, which is based on primary molding. The injection molding machine liquefies the plastic in granulate form.

Thermal insulation and thermal insulation materials – materials, practical knowledge, funding and future trends

Whenever objects with different temperatures are in physical contact or are in the area of radiant influences, heat exchange takes place.

Biomass: analysis, potential and industrial practice in the context of the energy transition

Biomass is one of the main pillars of the global energy transition and the development of sustainable materials. It comprises all organic matter of plant, animal or microbial origin that is present in a given ecosystem at a given time.

Analysis of thermoelectric materials – the figure of merit and its measurement

Thermoelectric materials can convert heat directly into electrical energy. This property is based on the Seebeck effect, in which a temperature difference applied to a material generates a voltage.

What does thermal conductivity mean?

In general, the thermal conductivity of the expression is the amount of heat that flows through a 1x1x1m cube of a material within 1 second if there is a temperature gradient of exactly 1 K between two opposite sides.

3D printing with metals – Thermal analyses

Metals are used almost everywhere in many industrial sectors for a wide variety of purposes.

Raman spectroscopy with DSC

Raman spectroscopy is a technique for investigating molecules and determining their structure and dynamics.

Determination of the CTE density

The thermal expansion of materials can lead to major economic damage. In the construction industry, for example, expansion joints must be provided to compensate for changes in length due to temperature fluctuations.

Thermal Impedance

Thermal management is a decisive factor in electronic devices, as overheating of components can lead to failures. The aim is therefore to transfer the heat generated by the electronics to a cooling device, e.g. a heat sink or heat sink.

Deformation techniques of metals

The deformation of metals is a crucial process in modern industry, with a wide range of applications from automotive manufacturing to aerospace.

Phase change analysis with DSC

What is a phase transition – Materials can be categorized and described in different ways. This can be based on their external appearance, certain physical parameters or more subjective impressions such as smell or taste.

DC and AC Hall Effect Measurements

The investigation of the Hall effect of a material is used specifically to determine the Hall coefficient as well as the charge carrier concentration, the charge carrier type and the mobility.

Polyamides: An Overview

Polyamides often present themselves as semi-crystalline materials with a mixture of ordered, crystalline structures and disordered, amorphous areas.

Martensitic transformations: The alchemy of hardness in metallurgy

There are few phenomena in the world of metallurgy that are as fascinating and at the same time as practical as martensitic transformation.

Phase transformations in metallurgy: a key to material innovation

Metallurgy is a science that is as old as civilization itself. Yet despite its ancient roots, it remains a field at the forefront of innovation.

High-density polyethylene (HDPE): An inside look

High-density polyethylene (HDPE) and polyethylene (PE) are both types of polyethylene, but they have different properties due to differences in production.

Endothermic vs. exothermic reactions

The main difference between exothermic and endothermic reactions lies in the heat exchange with the environment.

Polyethyleneterephthalate (PET): An in-depth investigation

Polyethylene terephthalate, commonly referred to as PET, occupies an important place in numerous industrial and commercial productions.

Polyvinyl chloride (PVC): An in-depth investigation

Polyvinyl chloride, also known as PVC, is a versatile thermoplastic that plays an important role in many industrial and commercial sectors.

Polystyrene (PS): A detailed analysis

Polystyrene, also known as polystyrene, is a widely used polymer produced by the polymerization of styrene.

Low density polyethylene (LDPE): A summary

Low density polyethylene, LDPE, is a thermoplastic polymer made from the monomer ethylene. It is a highly branched plastic.

Oxidation induction time and temperature

Oxidation is a chemical process that takes place when electrons are lost from a molecule, atom or ion.

Molten Salts – Heat transfer of the future

Molten salts are stable at high temperatures above 300 °C and exhibit remarkable thermal properties.

Acrylonitrile butadiene styrene (ABS): An in-depth look

Semiconductors with a larger energy gap (Eg) than conventional semiconductors, typically in the range above 2 eV, are referred to as wide bandgap semiconductors (WbGs).

Thermal Interface Materials – Heat Spreaders

Heat spreaders are thermally conductive objects that act as a bridge between a heat source and a heat exchanger.

Vespel™: The high-performance polymer revolutionizing extreme applications

Vespel™, developed by DuPont, is a high-performance polymer known for its ability to withstand extreme thermal, electrical and mechanical stresses.

Wide-Bandgap Semiconductors

Semiconductors with a larger energy gap (Eg) than conventional semiconductors, typically in the range above 2 eV, are referred to as Wide-Bandgap Semiconductors (WbG’s).