ASSISTENZA E SUPPORTO

Standard di analisi termica

Standard di analisi termica (ISO, ASTM e DIN)

Standard per il calorimetro a scansione differenziale

NORM

TITLE

ISO 11357Plastics - Differential scanning calorimetry (DSC) - Part 1: General principles (ISO 11357-1:2016)
ISO 11357Plastics - Differential scanning calorimetry (DSC) - Part 1: General principles (ISO 11357-1:2016)
ISO 11409Plastics - Phenolic resins - Determination of heat and reaction temperatures by differential scanning calorimetry (ISO 11409:1993); German version EN ISO 11409:1998
ISO 10837Determination of the thermal stability of polyethylene (PE) for use in gas pipes and fittings
DIN EN 728Plastics piping and ducting systems - Polyolefin pipes and fittings - Determination of oxidation induction time
DIN 65467Aerospace - Testing of thermoset resin systems with and without reinforcement - DSC method
ASTM E 794Standard test methods for melting and crystallization temperatures by thermal analysis
ASTM D 4565Standard test methods for physical and environmental performance characteristics of insulation and sheathing for telecommunication wires and cables
ASTM D 3895Standard test method for oxidation induction time of polyolefins by differential scanning calorimetry
ASTM C 351Standard Test Method for Mean Specific Heat of Thermal Insulation
ASTM E967Standard Test Method for Temperature Calibration of Differential Scanning Calorimeters and Differential Thermal Analyzers
ASTM E968Standard Practice for Heat Flow Calibration of Differential Scanning Calorimeters
ASTM E793Standard Test Method for Enthalpies of Fusion and Crystallization by Differential Scanning Calorimetry
ASTM D3895Standard Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning Calorimetry
ASTM D3417Standard Test Method for Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry (DSC) (Withdrawn 2004)
ASTM D3418Standard Test Method for Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry (DSC) (Withdrawn 2004)
ASTM E1269Standard Test Method for Determining Specific Heat Capacity by Differential Scanning Calorimetry
DIN 51004Thermal analysis (TA); determination of the melting temperatures of crystalline materials using differential thermal analysis (DTA)
DIN 51007Thermal Analysis (TA) - Differential Thermal Analysis (DTA) and Differential Scanning Calorimetry (DSC) - General Basics
DIN 53765Testing of plastics and elastomers; thermal analysis; differential scanning calorimetry (DSC)

Standard per la termogravimetria

NORM

TITLE

ISO 11358Plastics - Thermogravimetry (TG) of polymers - Part 1: General principles (ISO 11358-1:2014)
ISO 11358Plastics - Thermogravimetry (TG) of polymers - Part 1: General principles (ISO 11358-1:2014)
ISO 7111Plastics - Thermogravimetry of polymers - Temperature scanning method
DIN 51006Thermal analysis (TA) - Thermogravimetry (TG) - Fundamentals
ASTM E 914Practice for the evaluation of the temperature scale for thermogravimetry (withdrawn 1994)
ASTM E 1868Standard test methods for loss drying by thermogravimetry
ASTM D 3175Standard test methods for volatile substances in the analytical sample of coal and coke
ISO/DIS 9924Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry - Part 1: Butadiene, ethylene-propylene copolymer and terpolymer, isobutene-isoprene, isoprene and styrene-butadiene rubbers
ASTM E1131Standard Test Method for Compositional Analysis by Thermogravimetry
ASTM D3850Standard Test Method for Rapid Thermal Degradation of Solid Electrical Insulating Materials By Thermogravimetric Method (TGA)
ASTM D6375Standard Test Method for Evaporation Loss of Lubricating Oils by Thermogravimetric Analyzer (TGA) Noack Method
ASTM D6370Standard Test Method for Rubber—Compositional Analysis by Thermogravimetry (TGA)
ASTM E2550Standard Test Method for Thermal Stability by Thermogravimetry
ASTM D3175Standard Test Method for Volatile Matter in the Analysis Sample of Coal and Coke

Standard per l'analisi termomeccanica

NORM

TITLE

DIN 51005Thermal analysis (TA) - Terms
DIN 12667Thermal performance of building materials and products - Determination of thermal resistance by protected hot plate and heat flow meter methods - High and medium thermal resistance products; German version EN 12667:2001
ASTM D 3418Standard test methods for transition temperatures and enthalpies of fusion and crystallization of polymers by differential scanning calorimetry
ASTM D 3417Standard test methods for enthalpies of melting and crystallization of polymers by differential scanning calorimetry (DSC) (withdrawn 2004)
ISO 11359-2Plastics - Thermomechanical analysis (TMA) - Part 2: Determination of the coefficient of linear thermal expansion and glass transition temperature
IPC-TM-650 2.4.24Glass transition temperature and thermal expansion of the Z-axis using TMA
DIN 51005Thermal analysis (TA) - Terms
IPC-TM-650 2.4.41Linear coefficient of thermal expansion of electrical insulating materials
IPC-TM-650 2.4.24.1Time to delamination (TMA method)
IPC-TM-650 2.4.41.3Coefficient of thermal expansion in the plane, OrganicFilms
IPC-TM-650 2.4.24.3Glass transition temperature of organic films - TMA method
ENV 1159-3Advanced technical ceramics - Ceramic composites, thermophysical properties - Part 3: Determination of specific heat capacity
DIN 53752Testing of plastics; determination of the coefficient of linear thermal expansion
DIN 53545Testing of rubber - Determination of the low temperature behavior of elastomers - Principles and test methods
CEI/IEC 1006Test methods for determining the glass transition temperature of electrical insulating materials
ASTM E 2347Standard test method for indentation softening temperature by thermomechanical analysis
ASTM E 1824Standard test method for assigning a glass transition temperature by thermomechanical analysis: Tensile method
ASTM E 2113Standard test method for the extension calibration of thermomechanical analyzers
ASTM E 2092Standard test method for the deformation temperature at three-point bending by thermomechanical analysis
ASTM E 1545Standard test method for the determination of the glass transition temperature by thermomechanical analysis
ASTM D 3386Standard Test Method for Linear Thermal Expansion Coefficient of Electrical Insulating Materials1
ASTM E831Standard Test Method for Linear Thermal Expansion of Solid Materials by Thermomechanical Analysis
ASTM D696Standard Test Method for Coefficient of Linear Thermal Expansion of Plastics Between −30°C and 30°C with a Vitreous Silica Dilatometer
ISO 11359 – Parts 1 to 3Plastics — Thermomechanical analysis (TMA) — Part 3: Determination of penetration temperature
DIN 51045Determination of thermal expansion of solids - Part 1: Fundamentals

Standard per il dilatometro

NORM

TITLE

ASTM E831Standard Test Method for Linear Thermal Expansion of Solid Materials by Thermomechanical Analysis
ASTM A 1033Standard method for quantitative measurement and reporting of hypo-eutectoid carbon and low-alloy steel phase transformations
ASTM D696Standard Test Method for Coefficient of Linear Thermal Expansion of Plastics Between −30°C and 30°C with a Vitreous Silica Dilatometer
ASTM C372Standard Test Method for Linear Thermal Expansion of Porcelain Enamel and Glaze Frits and Fired Ceramic Whiteware Products by the Dilatometer Method
DIN 51045Determination of thermal expansion of solids - Part 1: Fundamentals

Standard per la conducibilità termica

NORM

TITLE

ASTM E1461Standard Test Method for Thermal Diffusivity by the Flash Method
DIN 30905Thermophysical properties of hard metals - Measurement of thermal diffusivity using the laser flash (heat pulse) method
JIS A 1412Test methods for thermal resistance and related properties of thermal insulation - Heat flux meter
ASTM D 5470Standard test method for thermal transmission properties of thermally conductive electrical insulation materials
DIN EN 821Advanced technical ceramics – Monolithic ceramics, thermo-physical properties – Part 2: Determination of thermal diffusity by the laser flash (or heat pulse) method
BS EN 1159-2Advanced technical ceramics. Ceramic composites. Thermophysical properties. Determination of thermal diffusivity
ASTM C714Standard Test Method for Thermal Diffusivity of Carbon and Graphite by Thermal Pulse Method
ASTM C518Standard Test Method for Steady-State Thermal Transmission Properties by Means of the Heat Flow Meter Apparatus
ISO 8301Thermal Insulation; Determination of Steady-State Thermal Transmission Resistance and Related Properties; Method Using the Heat Flow Meter Apparatus
DIN EN 12667 EN 12Thermal performance of building materials and products - Determination of thermal resistance by the plate apparatus and heat flow meter apparatus - High and medium thermal resistance products; German version EN 12667:2001

Servizio clienti

Il nostro servizio offre

Scegli tra le seguenti aree:

Manutenzione e riparazioni

Ti offriamo diversi servizi: Manutenzione, riparazioni, formazione e molto altro.

Assistenza remota

Un aiuto rapido e competente tramite Teamviewer? Puoi trovare istruzioni dettagliate qui

Applicazioni

Nella libreria delle applicazioni troverai alcune pubblicazioni con i nostri dispositivi di misurazione

Webinar

Clicca qui per una panoramica dei nostri webinar on-demand. Registrati e inizia!

Offerte speciali

Pacchetti di prodotti o offerte BOGO. Ti offriamo diversi pacchetti di risparmio!

Finanziamento dell'università

Supportiamo le università e i college nell’acquisizione di nuovi dispositivi di misurazione

Aiuto tramite il sito

Linea diretta di assistenza

Assistenza tecnica

Se hai bisogno di aiuto per risolvere problemi tecnici o hai domande sull’utilizzo del dispositivo, riceverai sempre una risposta rapida dalla nostra hotline di assistenza.

Il nostro servizio è disponibile dal lunedì al giovedì dalle 8.00 alle 16.00 e il venerdì dalle 8.00 alle 12.00.

Puoi anche scriverci utilizzando il modulo di contatto. Ti risponderemo entro un giorno lavorativo.

In questo modo potremo aiutarti nel più breve tempo possibile:

  • Tieni a portata di mano il numero di serie dell’apparecchio difettoso (vicino alla spina di rete sulla targhetta)
  • Indicaci dove si trova il dispositivo (città e paese)
  • Ti preghiamo di fornirci i tuoi recapiti per raggiungerti direttamente (e-mail e numero di telefono).