熱分析の規格(ISO、ASTM、DIN)
熱分析規格(ISO、ASTM、DIN)
示差走査熱量計の規格
NORM | TITLE |
|---|---|
| ISO 11357 | Plastics - Differential scanning calorimetry (DSC) - Part 1: General principles (ISO 11357-1:2016) |
| ISO 11357 | Plastics - Differential scanning calorimetry (DSC) - Part 1: General principles (ISO 11357-1:2016) |
| ISO 11409 | Plastics - Phenolic resins - Determination of heat and reaction temperatures by differential scanning calorimetry (ISO 11409:1993); German version EN ISO 11409:1998 |
| ISO 10837 | Determination of the thermal stability of polyethylene (PE) for use in gas pipes and fittings |
| DIN EN 728 | Plastics piping and ducting systems - Polyolefin pipes and fittings - Determination of oxidation induction time |
| DIN 65467 | Aerospace - Testing of thermoset resin systems with and without reinforcement - DSC method |
| ASTM E 794 | Standard test methods for melting and crystallization temperatures by thermal analysis |
| ASTM D 4565 | Standard test methods for physical and environmental performance characteristics of insulation and sheathing for telecommunication wires and cables |
| ASTM D 3895 | Standard test method for oxidation induction time of polyolefins by differential scanning calorimetry |
| ASTM C 351 | Standard Test Method for Mean Specific Heat of Thermal Insulation |
| ASTM E967 | Standard Test Method for Temperature Calibration of Differential Scanning Calorimeters and Differential Thermal Analyzers |
| ASTM E968 | Standard Practice for Heat Flow Calibration of Differential Scanning Calorimeters |
| ASTM E793 | Standard Test Method for Enthalpies of Fusion and Crystallization by Differential Scanning Calorimetry |
| ASTM D3895 | Standard Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning Calorimetry |
| ASTM D3417 | Standard Test Method for Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry (DSC) (Withdrawn 2004) |
| ASTM D3418 | Standard Test Method for Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry (DSC) (Withdrawn 2004) |
| ASTM E1269 | Standard Test Method for Determining Specific Heat Capacity by Differential Scanning Calorimetry |
| DIN 51004 | Thermal analysis (TA); determination of the melting temperatures of crystalline materials using differential thermal analysis (DTA) |
| DIN 51007 | Thermal Analysis (TA) - Differential Thermal Analysis (DTA) and Differential Scanning Calorimetry (DSC) - General Basics |
| DIN 53765 | Testing of plastics and elastomers; thermal analysis; differential scanning calorimetry (DSC) |
熱重量分析装置の規格
NORM | TITLE |
|---|---|
| ISO 11358 | Plastics - Thermogravimetry (TG) of polymers - Part 1: General principles (ISO 11358-1:2014) |
| ISO 11358 | Plastics - Thermogravimetry (TG) of polymers - Part 1: General principles (ISO 11358-1:2014) |
| ISO 7111 | Plastics - Thermogravimetry of polymers - Temperature scanning method |
| DIN 51006 | Thermal analysis (TA) - Thermogravimetry (TG) - Fundamentals |
| ASTM E 914 | Practice for the evaluation of the temperature scale for thermogravimetry (withdrawn 1994) |
| ASTM E 1868 | Standard test methods for loss drying by thermogravimetry |
| ASTM D 3175 | Standard test methods for volatile substances in the analytical sample of coal and coke |
| ISO/DIS 9924 | Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry - Part 1: Butadiene, ethylene-propylene copolymer and terpolymer, isobutene-isoprene, isoprene and styrene-butadiene rubbers |
| ASTM E1131 | Standard Test Method for Compositional Analysis by Thermogravimetry |
| ASTM D3850 | Standard Test Method for Rapid Thermal Degradation of Solid Electrical Insulating Materials By Thermogravimetric Method (TGA) |
| ASTM D6375 | Standard Test Method for Evaporation Loss of Lubricating Oils by Thermogravimetric Analyzer (TGA) Noack Method |
| ASTM D6370 | Standard Test Method for Rubber—Compositional Analysis by Thermogravimetry (TGA) |
| ASTM E2550 | Standard Test Method for Thermal Stability by Thermogravimetry |
| ASTM D3175 | Standard Test Method for Volatile Matter in the Analysis Sample of Coal and Coke |
熱機械分析装置の規格
NORM | TITLE |
|---|---|
| DIN 51005 | Thermal analysis (TA) - Terms |
| DIN 12667 | Thermal performance of building materials and products - Determination of thermal resistance by protected hot plate and heat flow meter methods - High and medium thermal resistance products; German version EN 12667:2001 |
| ASTM D 3418 | Standard test methods for transition temperatures and enthalpies of fusion and crystallization of polymers by differential scanning calorimetry |
| ASTM D 3417 | Standard test methods for enthalpies of melting and crystallization of polymers by differential scanning calorimetry (DSC) (withdrawn 2004) |
| ISO 11359-2 | Plastics - Thermomechanical analysis (TMA) - Part 2: Determination of the coefficient of linear thermal expansion and glass transition temperature |
| IPC-TM-650 2.4.24 | Glass transition temperature and thermal expansion of the Z-axis using TMA |
| DIN 51005 | Thermal analysis (TA) - Terms |
| IPC-TM-650 2.4.41 | Linear coefficient of thermal expansion of electrical insulating materials |
| IPC-TM-650 2.4.24.1 | Time to delamination (TMA method) |
| IPC-TM-650 2.4.41.3 | Coefficient of thermal expansion in the plane, OrganicFilms |
| IPC-TM-650 2.4.24.3 | Glass transition temperature of organic films - TMA method |
| ENV 1159-3 | Advanced technical ceramics - Ceramic composites, thermophysical properties - Part 3: Determination of specific heat capacity |
| DIN 53752 | Testing of plastics; determination of the coefficient of linear thermal expansion |
| DIN 53545 | Testing of rubber - Determination of the low temperature behavior of elastomers - Principles and test methods |
| CEI/IEC 1006 | Test methods for determining the glass transition temperature of electrical insulating materials |
| ASTM E 2347 | Standard test method for indentation softening temperature by thermomechanical analysis |
| ASTM E 1824 | Standard test method for assigning a glass transition temperature by thermomechanical analysis: Tensile method |
| ASTM E 2113 | Standard test method for the extension calibration of thermomechanical analyzers |
| ASTM E 2092 | Standard test method for the deformation temperature at three-point bending by thermomechanical analysis |
| ASTM E 1545 | Standard test method for the determination of the glass transition temperature by thermomechanical analysis |
| ASTM D 3386 | Standard Test Method for Linear Thermal Expansion Coefficient of Electrical Insulating Materials1 |
| ASTM E831 | Standard Test Method for Linear Thermal Expansion of Solid Materials by Thermomechanical Analysis |
| ASTM D696 | Standard Test Method for Coefficient of Linear Thermal Expansion of Plastics Between −30°C and 30°C with a Vitreous Silica Dilatometer |
| ISO 11359 – Parts 1 to 3 | Plastics — Thermomechanical analysis (TMA) — Part 3: Determination of penetration temperature |
| DIN 51045 | Determination of thermal expansion of solids - Part 1: Fundamentals |
ディラトメーターの規格
NORM | TITLE |
|---|---|
| ASTM E831 | Standard Test Method for Linear Thermal Expansion of Solid Materials by Thermomechanical Analysis |
| ASTM A 1033 | Standard method for quantitative measurement and reporting of hypo-eutectoid carbon and low-alloy steel phase transformations |
| ASTM D696 | Standard Test Method for Coefficient of Linear Thermal Expansion of Plastics Between −30°C and 30°C with a Vitreous Silica Dilatometer |
| ASTM C372 | Standard Test Method for Linear Thermal Expansion of Porcelain Enamel and Glaze Frits and Fired Ceramic Whiteware Products by the Dilatometer Method |
| DIN 51045 | Determination of thermal expansion of solids - Part 1: Fundamentals |
熱伝導率の標準
NORM | TITLE |
|---|---|
| ASTM E1461 | Standard Test Method for Thermal Diffusivity by the Flash Method |
| DIN 30905 | Thermophysical properties of hard metals - Measurement of thermal diffusivity using the laser flash (heat pulse) method |
| JIS A 1412 | Test methods for thermal resistance and related properties of thermal insulation - Heat flux meter |
| ASTM D 5470 | Standard test method for thermal transmission properties of thermally conductive electrical insulation materials |
| DIN EN 821 | Advanced technical ceramics – Monolithic ceramics, thermo-physical properties – Part 2: Determination of thermal diffusity by the laser flash (or heat pulse) method |
| BS EN 1159-2 | Advanced technical ceramics. Ceramic composites. Thermophysical properties. Determination of thermal diffusivity |
| ASTM C714 | Standard Test Method for Thermal Diffusivity of Carbon and Graphite by Thermal Pulse Method |
| ASTM C518 | Standard Test Method for Steady-State Thermal Transmission Properties by Means of the Heat Flow Meter Apparatus |
| ISO 8301 | Thermal Insulation; Determination of Steady-State Thermal Transmission Resistance and Related Properties; Method Using the Heat Flow Meter Apparatus |
| DIN EN 12667 EN 12 | Thermal performance of building materials and products - Determination of thermal resistance by the plate apparatus and heat flow meter apparatus - High and medium thermal resistance products; German version EN 12667:2001 |
カスタマーサービス
サービス内容
以下の分野からお選びください:
ヘルプ
サービス-ホットライン
リンザイスサービス-ホットライン
技術的な問題でお困りの場合や、デバイスの使用方法についてご質問がある場合は、当社のサービスホットラインからいつでも迅速に対応いたします。
月曜日から木曜日は午前8時から午後4時まで、金曜日は午前8時から午後12時までご利用いただけます。
お問い合わせフォームをご利用ください。
営業日以内にご返信いたします。
そうすることで、可能な限り迅速に対応することができます:
- 故障した電気器具の製造番号をお手元にご用意ください(定格銘板の主電源プラグの近く)。
- 電化製品が設置されている 場所(都市名と国名)をお知らせください。
- 直接連絡が取れる連絡先(Eメールと電話番号)をお知らせください。