德国林赛斯(LINSEIS Messgeräte GmbH)作为全球杰出的热物性分析设备生产商,可以更多满足客户对材料热物性评估的测试需求。我们的应用经验和能力完全可以满足您的测试需要。相比购买仪器来说,选择测试服务更为经济。测试结果将以表格和图形格式提供报告,并保存提供完整原始的测试数据。测试周期一般低于一周,且在测试完成后的数小时内通过电子邮件把结果发送给您。

测试说明:

如果需要样品测试服务,我们需要您提供样品的详细信息。请下载并填写该表格,与您的样品一同寄给我们。

 

1. Testing instructions (PDF Download)

2. Sample sheet (PDF Download)

Linseis Messgeräte GmbH
Vielitzerstr. 43
95100 Selb / Germany
Tel.: +49 (0) 9287/880 0
Fax: +49 (0) 9287/704 88
eMail: info@linseis.de

应用实验室提供的服务:

The following measurements can be offered as service in our application lab:


DIL – Dilatometry

  • Determination of coefficient of thermal expansion and thermal expansion between -150°C and 1750°C
  • Measurement from 275,- €
  • According to ASTM D 696, E 228, E 831, E 1363, E 1545, E 1824, DIN 53752

 

DSC – Dynamic scanning calorimetry

  • Measurement of enthalpy, phase transitions and specific heat capacity (Cp), Measurement from -150°C to 1550°C
  • Measurement from 250,- €
  • According to ASTM C 351, D 3417, D 3895, D 4565, E 793, E 794, DIN 51004, 51007, 53765, 65467, DIN EN 728, ISO 10837, 11357, 11409

 

TGA – Thermogravimetry

  • Measurement of mass change/ decomposition residues between RT and 1550°C
  • Measurement from 300,- €
  • According to ASTM E 914, E 1131, E 1868, DIN 51006, ISO 7111, 11358

 

STA – simultaneous thermal analysis

  • Simultaneous measurement of TG and DSC for determination of mass change and calorimetric effects between RT and 1550°C
  • Measurement from 350,- €
  • According to ASTM E 914, E 1131, E 1868, DIN 51006, ISO 7111, 11358

 

LFA - Laser Flash Analysis

  • Measurement of thermal diffusivity, thermal conductivity and sepcific heat capacity between RT and 1500°C
  • Measurement from 550,- €
  • According to ASTM E 1461, DIN 30905, DIN EN 821

 

THB - Transient Hot Bridge Measurement

  • Measurement of thermal conductivity between RT and 150°C
  • Measurement from 250,- €
  • According to ---

 

HFM – Heat flow meter

  • Measurement of thermal conductivity and thermal resistance (u-value) of insulators and insulation materials between 5°C and 80°C
  • Measurement from 300,- €
  • According to ASTM C518, JIS A 1412, ISO 8301, DIN 12667

 

LSR - Seebeck-, resistance- and ZT measurement

  • Measurement of seebeck-coefficient, electric conductivity / electric resistance and figure of merit (ZT) between RT and 1100°C
  • Measurement from 350,- €
  • According to JIS R 1650-1

 

RITA – inductive dilatometry

  • Measurement of phase diagrams and phase transitions of steel samples, CCT, CTT, TTT;
  • Measurement of coefficient of thermal expansion (CTE) with fast heating and cooling rates between RT and 1600°C
  • Measurement from 450,- €
  • According toASTM A1033-04

 

TF-LFA – thin film laser flash

  • Measurement of thermal diffusivity and thermal conductivity of thin films and coatings between RT and 500°C
  • Measurement from 1700.- €
  • According to ---