{"id":103285,"date":"2024-07-18T09:47:57","date_gmt":"2024-07-18T07:47:57","guid":{"rendered":"https:\/\/www.linseis.com\/sem-categoria\/impressao-3d-em-ceramica\/"},"modified":"2026-01-12T09:41:46","modified_gmt":"2026-01-12T08:41:46","slug":"impressao-3d-em-ceramica","status":"publish","type":"post","link":"https:\/\/www.linseis.com\/pt-pt\/conhecimentos\/impressao-3d-em-ceramica\/","title":{"rendered":"Impress\u00e3o 3D em cer\u00e2mica"},"content":{"rendered":"\t\t<div data-elementor-type=\"wp-post\" data-elementor-id=\"103285\" class=\"elementor elementor-103285 elementor-12087\" data-elementor-post-type=\"post\">\n\t\t\t\t<div class=\"elementor-element elementor-element-9eb8745 e-flex e-con-boxed e-con e-parent\" data-id=\"9eb8745\" data-element_type=\"container\" data-e-type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-6427b14 elementor-toc--minimized-on-tablet elementor-invisible elementor-widget elementor-widget-table-of-contents\" data-id=\"6427b14\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;headings_by_tags&quot;:[&quot;h2&quot;],&quot;exclude_headings_by_selector&quot;:[],&quot;_animation&quot;:&quot;fadeInUp&quot;,&quot;no_headings_message&quot;:&quot;No headings were found on this page.&quot;,&quot;marker_view&quot;:&quot;numbers&quot;,&quot;minimize_box&quot;:&quot;yes&quot;,&quot;minimized_on&quot;:&quot;tablet&quot;,&quot;hierarchical_view&quot;:&quot;yes&quot;,&quot;min_height&quot;:{&quot;unit&quot;:&quot;px&quot;,&quot;size&quot;:&quot;&quot;,&quot;sizes&quot;:[]},&quot;min_height_tablet&quot;:{&quot;unit&quot;:&quot;px&quot;,&quot;size&quot;:&quot;&quot;,&quot;sizes&quot;:[]},&quot;min_height_mobile&quot;:{&quot;unit&quot;:&quot;px&quot;,&quot;size&quot;:&quot;&quot;,&quot;sizes&quot;:[]}}\" data-widget_type=\"table-of-contents.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<div class=\"elementor-toc__header\">\n\t\t\t\t\t\t<h4 class=\"elementor-toc__header-title\">\n\t\t\t\t\u00cdndice\t\t\t<\/h4>\n\t\t\t\t\t\t\t\t\t\t<div class=\"elementor-toc__toggle-button elementor-toc__toggle-button--expand\" role=\"button\" tabindex=\"0\" aria-controls=\"elementor-toc__6427b14\" aria-expanded=\"true\" aria-label=\"Open table of contents\"><svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-chevron-down\" viewBox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M207.029 381.476L12.686 187.132c-9.373-9.373-9.373-24.569 0-33.941l22.667-22.667c9.357-9.357 24.522-9.375 33.901-.04L224 284.505l154.745-154.021c9.379-9.335 24.544-9.317 33.901.04l22.667 22.667c9.373 9.373 9.373 24.569 0 33.941L240.971 381.476c-9.373 9.372-24.569 9.372-33.942 0z\"><\/path><\/svg><\/div>\n\t\t\t\t<div class=\"elementor-toc__toggle-button elementor-toc__toggle-button--collapse\" role=\"button\" tabindex=\"0\" aria-controls=\"elementor-toc__6427b14\" aria-expanded=\"true\" aria-label=\"Close table of contents\"><svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-chevron-up\" viewBox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M240.971 130.524l194.343 194.343c9.373 9.373 9.373 24.569 0 33.941l-22.667 22.667c-9.357 9.357-24.522 9.375-33.901.04L224 227.495 69.255 381.516c-9.379 9.335-24.544 9.317-33.901-.04l-22.667-22.667c-9.373-9.373-9.373-24.569 0-33.941L207.03 130.525c9.372-9.373 24.568-9.373 33.941-.001z\"><\/path><\/svg><\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<div id=\"elementor-toc__6427b14\" class=\"elementor-toc__body\">\n\t\t\t<div class=\"elementor-toc__spinner-container\">\n\t\t\t\t<svg class=\"elementor-toc__spinner eicon-animation-spin e-font-icon-svg e-eicon-loading\" aria-hidden=\"true\" viewBox=\"0 0 1000 1000\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M500 975V858C696 858 858 696 858 500S696 142 500 142 142 304 142 500H25C25 237 238 25 500 25S975 237 975 500 763 975 500 975Z\"><\/path><\/svg>\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-8a9139e elementor-invisible elementor-widget elementor-widget-heading\" data-id=\"8a9139e\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">An\u00e1lise t\u00e9rmica de cer\u00e2micas impressas em 3D\n<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-ffaef65 elementor-invisible elementor-widget elementor-widget-text-editor\" data-id=\"ffaef65\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p><a href=\"https:\/\/www.linseis.com\/applikationen\/keramik-und-glas\/\">\n  <strong>A cer\u00e2mica<\/strong>\n<\/a> s\u00e3o utilizadas em muitas \u00e1reas da ind\u00fastria. Regra geral, as cer\u00e2micas s\u00e3o primeiro moldadas como um corpo verde a partir de mat\u00e9ria-prima, antes de este &#8220;corpo verde&#8221; ser tratado e cozido de uma forma especial (conhecida como sinteriza\u00e7\u00e3o) para o endurecer e lhe dar a sua forma final. <\/p><p>Dependendo da ind\u00fastria, pode tratar-se de lou\u00e7a simples, decora\u00e7\u00e3o ou lou\u00e7a sanit\u00e1ria, mas tamb\u00e9m de cer\u00e2mica t\u00e9cnica, como pr\u00f3teses ou v\u00e1rios componentes t\u00e9cnicos. Uma pe\u00e7a de cer\u00e2mica \u00e9 normalmente cozida num forno ap\u00f3s o processamento mec\u00e2nico inicial. \u00c9 exposta a temperaturas entre 900 \u00b0C e 1400 \u00b0C.  <\/p><p>Isto \u00e9 feito atrav\u00e9s do aquecimento, num intervalo de tempo definido, a uma temperatura em constante aumento, mas tamb\u00e9m em intervalos isot\u00e9rmicos precisamente definidos, de modo a controlar as reac\u00e7\u00f5es qu\u00edmicas durante a cozedura da cer\u00e2mica e a controlar a desgaseifica\u00e7\u00e3o do vapor de \u00e1gua, do di\u00f3xido de carbono e de outras misturas. Ap\u00f3s a primeira cozedura, \u00e9 frequentemente aplicado um esmalte na cer\u00e2mica e, em seguida, a pe\u00e7a \u00e9 novamente cozida para a endurecer completamente. <\/p><p>Todo o processo demora v\u00e1rias horas e, por conseguinte, envolve um tempo consider\u00e1vel. Al\u00e9m disso, n\u00e3o se pode garantir que a pe\u00e7a saia do forno intacta ap\u00f3s a cozedura; podem ocorrer v\u00e1rios erros (falta de material, processo de cozedura incorreto, etc.), que podem levar a quebras ou fissuras na cer\u00e2mica. <\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-4dbc798 elementor-widget elementor-widget-spacer\" data-id=\"4dbc798\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-d6d557b elementor-widget elementor-widget-spacer\" data-id=\"d6d557b\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-93f86bf elementor-widget elementor-widget-spacer\" data-id=\"93f86bf\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-104c7f5 elementor-invisible elementor-widget elementor-widget-text-editor\" data-id=\"104c7f5\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Uma solu\u00e7\u00e3o mais moderna e mais simples para a cozedura de uma grande variedade de componentes cer\u00e2micos \u00e9 o fabrico aditivo. No caso da cer\u00e2mica, isto \u00e9 muitas vezes referido como impress\u00e3o 3D. Trata-se de um processo de fabrico em que o material \u00e9 aplicado camada a camada para criar objectos tridimensionais.  <\/p><p>A constru\u00e7\u00e3o \u00e9 normalmente efectuada atrav\u00e9s de um desenho assistido por computador (CAD) e s\u00e3o utilizados um ou mais materiais l\u00edquidos ou s\u00f3lidos como material de base, de acordo com dimens\u00f5es e formas especificadas. Durante a constru\u00e7\u00e3o, atrav\u00e9s do processo de impress\u00e3o, ocorrem processos qu\u00edmicos <g id=\"gid_0\">\n  <g id=\"gid_1\">qu\u00edmicos ou processos de fus\u00e3o<\/g>\n<\/g> frequentemente controlados por temperatura ou laser. \u00c9 at\u00e9 poss\u00edvel utilizar um scanner 3D para um modelo.  <\/p><p>A vantagem deste m\u00e9todo em rela\u00e7\u00e3o aos processos de cozedura convencionais \u00e9 \u00f3bvia: a aplica\u00e7\u00e3o camada a camada da cer\u00e2mica permite a produ\u00e7\u00e3o de estruturas intrincadas e complexas, onde o risco de quebra durante o processo de cozedura seria particularmente elevado. Al\u00e9m disso, poupa imenso tempo, uma vez que uma pe\u00e7a sinterizada aditivamente ou impressa em 3D pode ser produzida muito mais rapidamente devido ao facto de n\u00e3o ser necess\u00e1rio o processo de cozedura no forno. <\/p><p>Em compara\u00e7\u00e3o com todos os processos de remo\u00e7\u00e3o de material, como corte, torneamento e perfura\u00e7\u00e3o, a impress\u00e3o 3D tem a vantagem de eliminar a etapa de processamento adicional ap\u00f3s o molde mestre. Na maioria dos casos, o processo tamb\u00e9m \u00e9 mais eficiente em termos energ\u00e9ticos, especialmente se o material s\u00f3 precisar de ser constru\u00eddo uma vez no tamanho e massa necess\u00e1rios. Tamb\u00e9m \u00e9 vantajoso que diferentes materiais possam ser processados numa \u00fanica m\u00e1quina.  <\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-df9d090 elementor-widget elementor-widget-spacer\" data-id=\"df9d090\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-5c4ab62 elementor-widget elementor-widget-spacer\" data-id=\"5c4ab62\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-967fcf7 elementor-widget elementor-widget-spacer\" data-id=\"967fcf7\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-7165763 e-con-full e-flex e-con e-child\" data-id=\"7165763\" data-element_type=\"container\" data-e-type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-9cd3e6a e-con-full e-flex e-con e-child\" data-id=\"9cd3e6a\" data-element_type=\"container\" data-e-type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-d6967c7 elementor-invisible elementor-widget elementor-widget-text-editor\" data-id=\"d6967c7\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Originalmente, o processo de impress\u00e3o 3D foi utilizado pela primeira vez na <a href=\"https:\/\/www.linseis.com\/applikationen\/polymere\/\">\n  <strong>ind\u00fastria dos pol\u00edmeros<\/strong>\n<\/a> uma vez que os pl\u00e1sticos s\u00e3o f\u00e1ceis de derreter e manusear e n\u00e3o requerem sinteriza\u00e7\u00e3o ou cura. Ao aquecer um pouco acima do ponto de amolecimento e arrefecer rapidamente o filamento impresso, as estruturas podiam ser criadas em tempo real. No entanto, o processo evoluiu rapidamente, de modo que n\u00e3o s\u00f3 v\u00e1rios pol\u00edmeros, mas tamb\u00e9m metais e cer\u00e2micas podem agora ser impressos, tornando a impress\u00e3o 3D uma op\u00e7\u00e3o vers\u00e1til para o fabrico.    <\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-97892db e-con-full e-flex e-con e-child\" data-id=\"97892db\" data-element_type=\"container\" data-e-type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-e84dc55 elementor-invisible elementor-widget elementor-widget-image\" data-id=\"e84dc55\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<img fetchpriority=\"high\" decoding=\"async\" width=\"800\" height=\"533\" src=\"https:\/\/www.linseis.com\/wp-content\/uploads\/2024\/07\/iStock-897850918-2048x1363-1-1-1024x682.jpg\" class=\"attachment-large size-large wp-image-34931\" alt=\"\" srcset=\"https:\/\/www.linseis.com\/wp-content\/uploads\/2024\/07\/iStock-897850918-2048x1363-1-1-1024x682.jpg 1024w, https:\/\/www.linseis.com\/wp-content\/uploads\/2024\/07\/iStock-897850918-2048x1363-1-1-300x200.jpg 300w, https:\/\/www.linseis.com\/wp-content\/uploads\/2024\/07\/iStock-897850918-2048x1363-1-1-768x511.jpg 768w, https:\/\/www.linseis.com\/wp-content\/uploads\/2024\/07\/iStock-897850918-2048x1363-1-1-1536x1022.jpg 1536w, https:\/\/www.linseis.com\/wp-content\/uploads\/2024\/07\/iStock-897850918-2048x1363-1-1.jpg 2048w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-0c82141 elementor-widget elementor-widget-spacer\" data-id=\"0c82141\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-49096c4 elementor-invisible elementor-widget elementor-widget-text-editor\" data-id=\"49096c4\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\tOs materiais t\u00edpicos atualmente utilizados na impress\u00e3o 3D incluem pl\u00e1sticos, cer\u00e2micas, metais e compostos de carbono, como a grafite. As t\u00e9cnicas mais importantes s\u00e3o a fus\u00e3o por feixe de laser e a fus\u00e3o por feixe de electr\u00f5es para os metais, a sinteriza\u00e7\u00e3o por laser para pol\u00edmeros, cer\u00e2micas e metais, a estereolitografia e o processamento digital de luz para resinas l\u00edquidas, bem como a modela\u00e7\u00e3o por polijacto e a modela\u00e7\u00e3o por camada fundida para pl\u00e1sticos e resinas. \t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-cc8c2be elementor-widget elementor-widget-spacer\" data-id=\"cc8c2be\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-5738a2c elementor-widget elementor-widget-spacer\" data-id=\"5738a2c\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-4433dc4 elementor-widget elementor-widget-spacer\" data-id=\"4433dc4\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-34a5387 e-con-full e-flex e-con e-child\" data-id=\"34a5387\" data-element_type=\"container\" data-e-type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-4f3901c e-con-full e-flex e-con e-child\" data-id=\"4f3901c\" data-element_type=\"container\" data-e-type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-891a9de elementor-invisible elementor-widget elementor-widget-text-editor\" data-id=\"891a9de\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Os processos de fabrico de aditivos podem ser divididos em sete categorias principais e s\u00e3o agora tamb\u00e9m descritos em pormenor em v\u00e1rias normas (DIN EN ISO\/ASTM 52900, anteriormente ASTM F2792):<\/p><ul><li>Sa\u00edda da pasta<\/li><li>Sa\u00edda de material<\/li><li>Fus\u00e3o de leito de p\u00f3<\/li><li>Extrus\u00e3o de materiais<\/li><li>Fotopolimeriza\u00e7\u00e3o em cuba<\/li><li>Deposi\u00e7\u00e3o de energia direcionada<\/li><li>Lamina\u00e7\u00e3o de folhas<\/li><\/ul>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-8c70769 e-con-full e-flex e-con e-child\" data-id=\"8c70769\" data-element_type=\"container\" data-e-type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-602a0ec elementor-invisible elementor-widget elementor-widget-image\" data-id=\"602a0ec\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" width=\"800\" height=\"449\" src=\"https:\/\/www.linseis.com\/wp-content\/uploads\/2024\/07\/IMG_5931-2048x1150-1-1-1024x575.jpg\" class=\"attachment-large size-large wp-image-34935\" alt=\"\" srcset=\"https:\/\/www.linseis.com\/wp-content\/uploads\/2024\/07\/IMG_5931-2048x1150-1-1-1024x575.jpg 1024w, https:\/\/www.linseis.com\/wp-content\/uploads\/2024\/07\/IMG_5931-2048x1150-1-1-300x168.jpg 300w, https:\/\/www.linseis.com\/wp-content\/uploads\/2024\/07\/IMG_5931-2048x1150-1-1-768x431.jpg 768w, https:\/\/www.linseis.com\/wp-content\/uploads\/2024\/07\/IMG_5931-2048x1150-1-1-1536x863.jpg 1536w, https:\/\/www.linseis.com\/wp-content\/uploads\/2024\/07\/IMG_5931-2048x1150-1-1.jpg 2048w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-fbaabd1 elementor-widget elementor-widget-spacer\" data-id=\"fbaabd1\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-cf94b06 elementor-widget elementor-widget-spacer\" data-id=\"cf94b06\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-fa70e7f elementor-widget elementor-widget-spacer\" data-id=\"fa70e7f\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-9a6bd63 elementor-invisible elementor-widget elementor-widget-text-editor\" data-id=\"9a6bd63\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>A principal diferen\u00e7a entre eles \u00e9 a forma como as camadas s\u00e3o aplicadas para produzir as pe\u00e7as e os materiais que s\u00e3o utilizados. Os factores mais importantes na escolha da m\u00e1quina e do processo de impress\u00e3o 3D s\u00e3o a velocidade (dependendo do tamanho do objeto) e o custo (do material e da m\u00e1quina). Materiais em geral: metal, cer\u00e2mica, pl\u00e1stico.  <br><br>A principal \u00e1rea de aplica\u00e7\u00e3o da tecnologia de fabrico aditivo continua a ser a investiga\u00e7\u00e3o e, sobretudo, o desenvolvimento de produtos e a constru\u00e7\u00e3o de prot\u00f3tipos na ind\u00fastria. \u00c9 ideal para a produ\u00e7\u00e3o de modelos, prot\u00f3tipos, ferramentas ou produtos espec\u00edficos, uma vez que n\u00e3o s\u00e3o necess\u00e1rias ferramentas especiais e a convers\u00e3o do desenho para o modelo pode ser efectuada muito rapidamente. <br><br>Outras \u00e1reas de aplica\u00e7\u00e3o incluem a tecnologia m\u00e9dica, em particular, onde pr\u00f3teses e implantes especialmente personalizados (especialmente em medicina dent\u00e1ria) t\u00eam frequentemente de ser feitos \u00e0 medida. No entanto, \u00e1reas de aplica\u00e7\u00e3o mais invulgares, como a escultura e a arte, tamb\u00e9m utilizam o fabrico aditivo para a produ\u00e7\u00e3o de esculturas. Atualmente, as impressoras 3D tamb\u00e9m podem ser utilizadas para fins privados, uma vez que os processos e as impressoras est\u00e3o prontos para a produ\u00e7\u00e3o em s\u00e9rie e est\u00e3o dispon\u00edveis ao p\u00fablico a um custo relativamente baixo. No sector dom\u00e9stico, os produtos de pl\u00e1stico, como brinquedos, pe\u00e7as sobressalentes ou pequenos suportes, podem ser produzidos facilmente e sem grandes conhecimentos pr\u00e9vios.   <\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-b869321 elementor-invisible elementor-widget elementor-widget-heading\" data-id=\"b869321\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">Os seguintes m\u00e9todos de impress\u00e3o 3D s\u00e3o utilizados para cer\u00e2mica:\n<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-03bc60f elementor-invisible elementor-widget elementor-widget-text-editor\" data-id=\"03bc60f\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<ul><li>Processos de fus\u00e3o em leito de p\u00f3, como a sinteriza\u00e7\u00e3o selectiva por laser (SLS).<ul><li>Este processo pode geralmente ser utilizado para imprimir pol\u00edmeros, p\u00f3s cer\u00e2micos ou metais. O material em p\u00f3 \u00e9 fundido com um laser de alta energia para produzir materiais completamente densos, camada a camada. Uma fina camada de p\u00f3 \u00e9 depositada num tabuleiro utilizando um bocal. Em seguida, um laser come\u00e7a a sinterizar o p\u00f3 localmente, criando a primeira camada. Uma varia\u00e7\u00e3o deste processo \u00e9 a impress\u00e3o 3D a jato de tinta. Aqui, um aglutinante \u00e9 impresso numa camada de p\u00f3 (gesso ou resina) na sec\u00e7\u00e3o transversal da pe\u00e7a, utilizando um processo semelhante \u00e0 impress\u00e3o a jato de tinta. Uma vantagem das t\u00e9cnicas de fus\u00e3o em leito de p\u00f3 \u00e9 que o excesso de p\u00f3 serve de suporte para o objeto impresso.      <\/li><\/ul><\/li><\/ul>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-cf18a83 elementor-widget elementor-widget-spacer\" data-id=\"cf18a83\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-d6b4905 elementor-widget elementor-widget-spacer\" data-id=\"d6b4905\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-3d6a78f elementor-invisible elementor-widget elementor-widget-text-editor\" data-id=\"3d6a78f\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<ul><li>Na modela\u00e7\u00e3o por deposi\u00e7\u00e3o fundida (FDM) ou no fabrico por filamento fundido (FFF), s\u00e3o processadas pequenas part\u00edculas da cer\u00e2mica desejada.<ul><li>Para que isto funcione, \u00e9 utilizado um aglutinante espec\u00edfico no filamento, normalmente um pl\u00e1stico especial que mant\u00e9m o p\u00f3 cer\u00e2mico unido.<\/li><li>O filamento \u00e9 depois aquecido de tal forma que se liquefaz e pode ser impresso, tal como um filamento de pl\u00e1stico convencional. Os gr\u00e3os de cer\u00e2mica t\u00eam aqui um di\u00e2metro de cerca de 1-2 \u00b5m. <ul><li>Como resultado, saem diretamente do bocal ao imprimir com o pl\u00e1stico e as camadas desejadas podem ser impressas diretamente.<\/li><li>Apenas o pl\u00e1stico que segura e transporta o p\u00f3 em conjunto derrete durante este processo, servindo assim como agente aglutinante.<ul><li>No final, \u00e9 criado um molde impresso, mas que continua a ser essencialmente constitu\u00eddo pelo p\u00f3 cer\u00e2mico e n\u00e3o por um corpo cer\u00e2mico s\u00f3lido.<\/li><\/ul><\/li><\/ul><\/li><li>Este n\u00e3o \u00e9 ainda o produto final, mas um produto verde que ainda precisa de ser reformulado.<ul><li>Finalmente, parte do pl\u00e1stico \u00e9 removido atrav\u00e9s de um processo especial. Segue-se o processo de sinteriza\u00e7\u00e3o, no qual a pe\u00e7a \u00e9 exposta a altas temperaturas e subst\u00e2ncias qu\u00edmicas num forno especial. <\/li><li>As pe\u00e7as cer\u00e2micas unem-se e o pl\u00e1stico \u00e9 completamente removido. Isto significa que o FDM \u00e9, em \u00faltima an\u00e1lise, muito semelhante ao processo original de cozedura de cer\u00e2mica, uma vez que apenas se poupa um passo de cozedura, mas o segundo continua a ter de ser efectuado. <\/li><\/ul><\/li><\/ul><\/li><\/ul>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-c74ffa0 elementor-widget elementor-widget-spacer\" data-id=\"c74ffa0\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-3f0c409 elementor-widget elementor-widget-spacer\" data-id=\"3f0c409\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-16ca4d1 elementor-invisible elementor-widget elementor-widget-text-editor\" data-id=\"16ca4d1\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>As condi\u00e7\u00f5es corretas para o material a utilizar numa impressora 3D dependem do comportamento t\u00e9rmico, como a temperatura de fus\u00e3o e a forma como o material se expande sob a a\u00e7\u00e3o da temperatura ou a condutividade t\u00e9rmica presente. Por isso, faz sentido testar exaustivamente as propriedades t\u00e9rmicas dos materiais utilizados na impress\u00e3o 3D. Os seguintes dispositivos s\u00e3o relevantes para estes testes:  <\/p><ul><li>Com a cl\u00e1ssica <a href=\"https:\/\/www.linseis.com\/methoden\/dilatometrie\/\">\n  <strong>dilatometria (DIL)<\/strong>\n<\/a> pode ser utilizado para investigar extensivamente a expans\u00e3o linear t\u00e9rmica e o comportamento de sinteriza\u00e7\u00e3o de s\u00f3lidos e p\u00f3s. Isto significa que a dilatometria \u00e9 atualmente um procedimento padr\u00e3o na produ\u00e7\u00e3o de cer\u00e2mica. <\/li><li>Al\u00e9m disso, v\u00e1rios m\u00e9todos de an\u00e1lise da condutividade t\u00e9rmica s\u00e3o \u00fateis para simular e controlar a distribui\u00e7\u00e3o e a condu\u00e7\u00e3o da temperatura na pe\u00e7a de trabalho. Os m\u00e9todos mais comuns neste dom\u00ednio s\u00e3o as t\u00e9cnicas de flash, como o <g id=\"gid_0\">\n  <g id=\"gid_1\">m\u00e9todo de flash laser (LFA)<\/g>\n<\/g> em que a temperatura e a condutividade t\u00e9rmica de s\u00f3lidos ou p\u00f3s podem ser medidas utilizando um flash de luz de alta energia. Existem tamb\u00e9m m\u00e9todos de fio quente, como o m\u00e9todo <g id=\"gid_2\">\n  <g id=\"gid_3\">ponte quente transiente (THB)<\/g>\n<\/g>que podem fornecer valores fi\u00e1veis de transfer\u00eancia de calor de forma relativamente r\u00e1pida \u00e0 temperatura ambiente. Para pastas e p\u00f3s, o <a href=\"https:\/\/www.linseis.com\/messgeraete\/waermeleitfaehigkeit\/tim-l58\/\">\n  <strong>Trans Interface Material Tester (TIM)<\/strong>\n<\/a>uma modifica\u00e7\u00e3o da <a href=\"https:\/\/www.linseis.com\/methoden\/guarded-hot-plate-ghp\/\">\n  <strong>placa quente protegida<\/strong>\n<\/a>que pode medir diferentes densidades aparentes e as altera\u00e7\u00f5es resultantes nas propriedades de transporte t\u00e9rmico.   <\/li><\/ul>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-03a0372 elementor-widget elementor-widget-spacer\" data-id=\"03a0372\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-49f6deb elementor-widget elementor-widget-spacer\" data-id=\"49f6deb\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-db736d4 elementor-widget elementor-widget-spacer\" data-id=\"db736d4\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-2368ff1 elementor-invisible elementor-widget elementor-widget-text-editor\" data-id=\"2368ff1\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Depois de um componente ter sido fabricado, \u00e9 importante determinar os requisitos para o componente em termos de propriedades t\u00e9rmicas e mec\u00e2nicas e desenvolv\u00ea-los com um design especificamente adaptado ao processo. Isto aplica-se normalmente independentemente do processo de fabrico utilizado para produzir o componente. No caso de componentes fabricados aditivamente, no entanto, \u00e9 particularmente necess\u00e1rio verificar as propriedades mec\u00e2nicas, uma vez que estas podem diferir das de um objeto moldado ou cozido devido \u00e0 estrutura da camada. Particularmente no caso da cer\u00e2mica, a pe\u00e7a de trabalho encolhe massivamente ap\u00f3s a sinteriza\u00e7\u00e3o ou aplica\u00e7\u00e3o de aditivos e pode haver v\u00e1rias fontes de defeitos que levam \u00e0 falha do material. Tamb\u00e9m aqui \u00e9 geralmente utilizado um dilat\u00f3metro e, em alguns casos, at\u00e9 mesmo a an\u00e1lise termomec\u00e2nica (TMA), que \u00e9 capaz de registar com precis\u00e3o as propriedades mec\u00e2nicas do material atrav\u00e9s de ensaios de flex\u00e3o, tra\u00e7\u00e3o e compress\u00e3o.    <\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-ccc9372 elementor-widget elementor-widget-spacer\" data-id=\"ccc9372\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t","protected":false},"excerpt":{"rendered":"<p>A cer\u00e2mica \u00e9 utilizada em muitas \u00e1reas da ind\u00fastria. Regra geral, as cer\u00e2micas s\u00e3o primeiro moldadas como corpos verdes a partir de massa bruta, antes de este &#8220;corpo verde&#8221; ser tratado e cozido de uma forma especial (a chamada sinteriza\u00e7\u00e3o). <\/p>\n","protected":false},"author":3,"featured_media":32789,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"inline_featured_image":false,"footnotes":""},"categories":[654],"tags":[],"class_list":["post-103285","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-conhecimentos"],"acf":[],"_links":{"self":[{"href":"https:\/\/www.linseis.com\/pt-pt\/wp-json\/wp\/v2\/posts\/103285","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.linseis.com\/pt-pt\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.linseis.com\/pt-pt\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.linseis.com\/pt-pt\/wp-json\/wp\/v2\/users\/3"}],"replies":[{"embeddable":true,"href":"https:\/\/www.linseis.com\/pt-pt\/wp-json\/wp\/v2\/comments?post=103285"}],"version-history":[{"count":0,"href":"https:\/\/www.linseis.com\/pt-pt\/wp-json\/wp\/v2\/posts\/103285\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.linseis.com\/pt-pt\/wp-json\/wp\/v2\/media\/32789"}],"wp:attachment":[{"href":"https:\/\/www.linseis.com\/pt-pt\/wp-json\/wp\/v2\/media?parent=103285"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.linseis.com\/pt-pt\/wp-json\/wp\/v2\/categories?post=103285"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.linseis.com\/pt-pt\/wp-json\/wp\/v2\/tags?post=103285"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}