{"id":101653,"date":"2024-07-22T08:54:47","date_gmt":"2024-07-22T06:54:47","guid":{"rendered":"https:\/\/www.linseis.com\/bez-kategorii\/pomiar-przejsc-fazowych-za-pomoca-dylatometru\/"},"modified":"2026-01-16T10:04:43","modified_gmt":"2026-01-16T09:04:43","slug":"pomiar-przejsc-fazowych-za-pomoca-dylatometru","status":"publish","type":"post","link":"https:\/\/www.linseis.com\/pl\/wiedza\/pomiar-przejsc-fazowych-za-pomoca-dylatometru\/","title":{"rendered":"Pomiar przej\u015b\u0107 fazowych za pomoc\u0105 dylatometru"},"content":{"rendered":"\t\t<div data-elementor-type=\"wp-post\" data-elementor-id=\"101653\" class=\"elementor elementor-101653 elementor-14718\" data-elementor-post-type=\"post\">\n\t\t\t\t<div class=\"elementor-element elementor-element-9eb8745 e-flex e-con-boxed e-con e-parent\" data-id=\"9eb8745\" data-element_type=\"container\" data-e-type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-ffaef65 elementor-invisible elementor-widget elementor-widget-text-editor\" data-id=\"ffaef65\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Dylatometr mo\u017ce by\u0107 wykorzystywany do okre\u015blania przej\u015b\u0107 fazowych w materia\u0142ach, poniewa\u017c zmiana fazy jest r\u00f3wnie\u017c zwi\u0105zana ze zmian\u0105 wsp\u00f3\u0142czynnika rozszerzalno\u015bci cieplnej (CTE). <a href=\"https:\/\/www.linseis.com\/startseite\/messgroessen\/laengenausdehnungskoeffizient\/\">\n  <strong>wsp\u00f3\u0142czynnik rozszerzalno\u015bci cieplnej (CTE)<\/strong>\n<\/a> materia\u0142u. Temperatura, w kt\u00f3rej zmienia si\u0119 CTE, jest znana jako temperatura przej\u015bcia fazowego. Opr\u00f3cz pomiaru wsp\u00f3\u0142czynnika rozszerzalno\u015bci cieplnej, dylatometr typu TMA (<a href=\"https:\/\/www.linseis.com\/startseite\/methoden\/thermomechanische-analyse\/\">\n  <strong>analiza termomechaniczna<\/strong>\n<\/a>) umo\u017cliwia pomiar w\u0142a\u015bciwo\u015bci mechanicznych. Mo\u017cna go r\u00f3wnie\u017c wykorzysta\u0107 do identyfikacji zmian fazowych, poniewa\u017c w\u0142a\u015bciwo\u015bci mechaniczne, takie jak modu\u0142 spr\u0119\u017cysto\u015bci, r\u00f3wnie\u017c zmieniaj\u0105 si\u0119 podczas przej\u015b\u0107 fazowych.   <\/p><p>Dylatometr <a href=\"https:\/\/www.linseis.com\/messgeraete\/dilatometer\/dil-l78-abschreckdilatometer\/\">\n  <strong>Dylatometr hartowniczy Linseis L78<\/strong>\n<\/a> jest powszechnie stosowany do pomiaru temperatur przemian fazowych (austenit, ferryt, martenzyt, perlit, baindt itp.) w stalach. Ten typ dylatometru pr\u0119towego pomaga symulowa\u0107 metody produkcji, takie jak obr\u00f3bka cieplna w k\u0105pieli solnej, hartowanie w k\u0105pieli olejowej itp. <\/p><p>Te temperatury transformacji zmieniaj\u0105 si\u0119 w zale\u017cno\u015bci od szybko\u015bci ogrzewania i ch\u0142odzenia. W przypadku niekt\u00f3rych przej\u015b\u0107 fazowych wymagane s\u0105 wysokie szybko\u015bci ogrzewania i ch\u0142odzenia. Szybko\u015b\u0107 ta jest generowana przez nagrzewnic\u0119 indukcyjn\u0105 i cewk\u0119 indukcyjn\u0105 z cewk\u0105 ch\u0142odz\u0105c\u0105 gaz. Na przyk\u0142ad, pr\u00f3bka mo\u017ce zosta\u0107 podgrzana do 1000 \u00b0C i sch\u0142odzona do temperatury pokojowej w czasie kr\u00f3tszym ni\u017c 30 sekund.   <\/p><p>Dzi\u0119ki rozszerzeniu odkszta\u0142cenia, do pr\u00f3bki mo\u017cna przy\u0142o\u017cy\u0107 si\u0142\u0119 osiow\u0105 w celu symulacji proces\u00f3w utwardzania napr\u0119\u017ceniowego. Dzi\u0119ki temu dylatometrowi naukowcy mog\u0105 <g id=\"gid_0\">tworzy\u0107 wykresy CCT i TTT<\/g> oraz opracowywa\u0107 nowe <g id=\"gid_1\">kompozycje metali<\/g>. Diagramy te pomagaj\u0105 zoptymalizowa\u0107 procedury przetwarzania, kt\u00f3re mo\u017cna wykorzysta\u0107 do uzyskania po\u017c\u0105danego sk\u0142adu wielofazowego w stopie metalu, kt\u00f3ry nadaje mu unikalne w\u0142a\u015bciwo\u015bci mechaniczne.  <\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-0b6c6aa elementor-widget elementor-widget-spacer\" data-id=\"0b6c6aa\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-0723713 elementor-widget elementor-widget-spacer\" data-id=\"0723713\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-8d64dd9 elementor-invisible elementor-widget elementor-widget-text-editor\" data-id=\"8d64dd9\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;_animation&quot;:&quot;fadeInUp&quot;}\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Temperatura zeszklenia <a href=\"https:\/\/www.linseis.com\/pl\/wiedza\/temperatura-zeszklenia\/\">\n  <strong>Temperatura zeszklenia Tg<\/strong>\n<\/a> mo\u017cna zmierzy\u0107 dla materia\u0142\u00f3w niekrystalicznych, takich jak szk\u0142a lub polimery, za pomoc\u0105 dylatometru. Temperatura ta wyznacza punkt, w kt\u00f3rym ruchy molekularne gwa\u0142townie wzrastaj\u0105 i rozpoczyna si\u0119 transformacja materia\u0142u ze stanu sta\u0142ego do gumowatego, lepkospr\u0119\u017cystego. W temperaturze zeszklenia wsp\u00f3\u0142czynnik CTE wzrasta i mo\u017cna go zmierzy\u0107 jako zmian\u0119 nachylenia krzywej rozszerzalno\u015bci. Je\u015bli pr\u00f3bka jest dalej podgrzewana, krzywa rozszerzalno\u015bci osi\u0105ga maksimum w punkcie mi\u0119knienia. Nast\u0119pnie lepko\u015b\u0107 spada i pr\u00f3bka zaczyna p\u0142yn\u0105\u0107. TMA mo\u017ce r\u00f3wnie\u017c wykorzysta\u0107 spadek modu\u0142u spr\u0119\u017cysto\u015bci do okre\u015blenia Tg.     <\/p><p>Dylatometry Linseis s\u0105 wyposa\u017cone w funkcj\u0119 wykrywania punktu mi\u0119kni\u0119cia, kt\u00f3ra automatycznie zatrzymuje nagrzewanie pieca po osi\u0105gni\u0119ciu punktu mi\u0119kni\u0119cia. Pomaga to zapobiec stopieniu si\u0119 materia\u0142\u00f3w w urz\u0105dzeniu i zniszczeniu systemu pomiarowego. <\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-5a561c0 elementor-widget elementor-widget-spacer\" data-id=\"5a561c0\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"spacer.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div class=\"elementor-spacer\">\n\t\t\t<div class=\"elementor-spacer-inner\"><\/div>\n\t\t<\/div>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t","protected":false},"excerpt":{"rendered":"<p>Dylatometr mo\u017ce by\u0107 wykorzystywany do okre\u015blania przej\u015b\u0107 fazowych w materia\u0142ach, poniewa\u017c zmianie fazy towarzyszy r\u00f3wnie\u017c zmiana wsp\u00f3\u0142czynnika rozszerzalno\u015bci cieplnej (CTE) materia\u0142u.  <\/p>\n","protected":false},"author":3,"featured_media":33535,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"inline_featured_image":false,"footnotes":""},"categories":[596],"tags":[],"class_list":["post-101653","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-wiedza"],"acf":[],"_links":{"self":[{"href":"https:\/\/www.linseis.com\/pl\/wp-json\/wp\/v2\/posts\/101653","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.linseis.com\/pl\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.linseis.com\/pl\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.linseis.com\/pl\/wp-json\/wp\/v2\/users\/3"}],"replies":[{"embeddable":true,"href":"https:\/\/www.linseis.com\/pl\/wp-json\/wp\/v2\/comments?post=101653"}],"version-history":[{"count":0,"href":"https:\/\/www.linseis.com\/pl\/wp-json\/wp\/v2\/posts\/101653\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.linseis.com\/pl\/wp-json\/wp\/v2\/media\/33535"}],"wp:attachment":[{"href":"https:\/\/www.linseis.com\/pl\/wp-json\/wp\/v2\/media?parent=101653"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.linseis.com\/pl\/wp-json\/wp\/v2\/categories?post=101653"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.linseis.com\/pl\/wp-json\/wp\/v2\/tags?post=101653"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}