TGA PT1000 (TGA Thermogravimetry / Thermal Balance)

Cost effective Thermobalance (Thermogravimetric Analyzer)

[Translate to Korea:] The NEW Linseis TGA PT1000 for thermogravimetric applications is a toploading Thermobalance, which offers a highly userfriendly design. Even at a sample weight of up to 5g the tara is done electronically. The specially designed furnaces allow fast heating and cooling rates from 0.01 up to 150°C/min as well as a highly precise temperature control from RT up to 1100°C. The system can be optionally equipped with a coupling device for EGA (Evolved Gas Analysis). The instrument is highly suitable for thermal composition, thermal stability and oxidation studies. The (optional) calculated DTA signal provides important additional information regarding endothermal or exothermal reactions. Furthermore it can be used as a tool for temperature calibration.

NEW Linseis automation system:

An optional 20 position sample robot in combination with the optional automatic gas control and automatic evacuating system enables long term unattended operation.

For an even higher throughput, a sample robot for up to 64 positions is also available.

    [Translate to Korea:]

    Model: TGA PT1000 TGA PT1000 HiRes 
    Temperature range: RT up to 1100°C RT up to 1100°C
    Heating and Cooling rates: 0.01 to 150°C/min 0.001 to 200°C/min
    Sample mass: up to 5g up to 2g
    Resolution: 0.5 µg 0.1 µg
    Vacuum: - Yes (optional)
    Cool down speed: < 15min (1100°C – 100°C) < 15min (1100°C – 100°C)
    Sample Carriers: TGA TGA-DTA/DSC*
    Sample Robot: 44 Positions 88 Positions
    Electronics: integrated integrated
    Interface: USB USB

    *calculated DTA/DSC

      [Translate to Korea:] All LINSEIS thermo analytical instruments are PC controlled. The individual software modules exclusively run under Microsoft® Windows® operating systems. The complete software consists of 3 modules: temperature control, data acquisition and data evaluation. The 32 bit software incorporates all essential features for measurement preparation, execution, and evaluation of a Thermogravimetric measurement. Thanks to our specialists and application experts, LINSEIS was able to develop comprehensive easy to understand user friendly application software.

      General Features

      • Program capable of text editing
      • Data security in case of power failure
      • Thermocouple break protection
      • Repetition measurements with minimum parameter input
      • Evaluation of current measurement
      • Curve comparison up to 32 curves
      • Storage and export of evaluations
      • Export and import of data ASCII
      • Data export to MS Excel
      • Multi-methods analysis (DSC TG, TMA, DIL, etc.)
      • Zoom function
      • 1 and 2 derivation
      • Programmable gas control
      • Statistical evaluation package
      • Free scaling

      TG – Features

      • Mass change as % and mg
      • Rate Controlled Mass Loss
      • Evaluation of mass loss
      • Residue mass evaluation

        [Translate to Korea:]

        Materials

        Polymers, Organics

        Industries

        Automotive / Aviation / Aerospace, Research, Development and Academia, Cosmetics, Pharmaceuticals and Food Industry, Chemical, Electronics Industry

        Determination of quantity of chalk of a PE-foil

        The pyrolisis starts at approx. 400°C under conditions almost free of oxygen. The chalk which is added as fill stuff splits off at a temperature of approximately 600°C. You can determine the quantity of chalk from the lost of weight. You can determine the content of chalk to 55,4 %, if there was pure chalk.

          [Translate to Korea:] Here is a short extract of our available accessories:

            • Software for determination of calculated DTA signal
            • Different types of vacuum and turbo molecular pumps
            • Selection of manual, semi-automatic and automatic (MFC) Gas control boxes
            • Broad range of crucibles (gold, silver, platinum, quartz glass, alumina oxide, aluminum, high pressure stainless steel, etc.)