DIL L75 Laser

Highest Precision Laser Dilatometer

Description

On point

Unmatched resolution and absolute accuracy is now possible due to the development of the Linseis Laser Dilatometer of the Pico-series. As the name indicates already the resolution goes up to Picometers (0,3 nm = 300 Picometer). That means resolutions can be obtained which are up to a factor 33,33 higher as the resolution that were possible up to date.

On top the principle of interference measurement give the possibility for much higher accuracy’s, especially as some special computer calibrations are used.

Linseis L75/LASER only needs slight machining of the sample. All you need to do is just prepare one sample, as with the conventional push rod type dilatometer. The system does not require any specific sample geometry. All types of material, reflecting or none reflecting can be evaluated with the system.

The measurement principle is an “absolute measurement”, not like conventional double sample pushrod Dilatometers, providing much higher precision. No calibration has to be undertake, unlike with conventional Dilatometers.

 

You are interested in a instrument?

You need more information?

Contact us today!

 

Send us your request >>

Specifications

Dilatometer L 75 Querschnitt

Model DIL L75 Laser *
Temperature range: -180 bis 500°C
RT … 1000°C
Resolution: 0.3 nm
Heating/cooling rates: 0.01 K/min … 50 K/min
Sample holders: fused silica
Sample length: up to 20 mm
Sample diameter: up to ∅ 7 mm
Atmosphere: inert, oxic., red., vac.
Interface: USB

*Specs depend on configurations

Accessories

Measuring systems Dilatometers

  • Sample preparation devices
  • Different types of vacuum and turbomolecular pumps
  • Different types (designs/materials) of sample holders
  • Vernier calipers for online input of the sample length
  • Selection of Gas Boxes for up to 4 gases

Software

All LINSEIS thermo analytical instruments are PC controlled. The individual software modules exclusively run under Microsoft® Windows® operating systems. The complete software consists of 3 modules: temperature control, data acquisition and data evaluation. The 32 bit software incorporates all essential features for measurement preparation, execution, and evaluation of a Dilatometer measurement. Thanks to our specialists and application experts, LINSEIS was able to develop comprehensive easy to understand user friendly application software.

DIL-Features

  • Glass transition and softening point evaluation
  • Softening point detection with automatic software controlled system shut down
  • Display of relative/absolute shrinkage or expansion curves
  • Presentation and calculation of technical / physical expansion coefficient
  • Rate Controlled Sintering (RCS) Software
  • Sinter process evaluation
  • Semiautomatic evaluation functions
  • Several system correction features
  • Automatic zero point adjustment

 

General Features

  • Program capable of text editing
  • Data security in case of power failure
  • Thermocouple break protection
  • Repetition measurements with minimum parameter input
  • Evaluation of current measurement
  • Curve comparison up to 32 curves
  • Storage and export of evaluations
  • Export and import of data ASCII
  • Data export to MS Excel
  • Multi-methods analysis (DSC TG, TMA, DIL, etc.)
  • Zoom function
  • 1 and 2 derivation
  • Programmable gas control
  • Statistical evaluation package
  • Free scaling

Applications

Application example: Invar

An INVAR sample was evaluated four times during heating in an air atmosphere. The temperature range was room temperature up to 200°C. This comparison clearly demonstrates the unbeaten accuracy of the LASER measuring technique. The difference of the four measurements is as low as 0.01% FS. With the patented LINSEIS Laser Dilatometer, resolutions can be obtained which are up to a factor 33 higher than the resolution possible up to date with a conventional Dilatometer.

Dilatomer Laser Applikation Invar