Programas de dilatometros de hornos

Horizontal Rule
 
     
Temperaturas entre: -150°C - 500°C  Temperaturas entre: 20°C - 1000°C  Temperaturas entre: 20°C - 1250°C 
     
Temperaturas entre: 20°C - 1550°C  Temperaturas entre: 20°C - 1750°C  Temperaturas entre: 20°C - 2300°C 
 
 
Horizontal
Temperatura  Tipo  Elemento  Variacion en 
Temp. 
Atmosfera Enfriador Tipo TC 
20°C-1000°C  L75/220  Kanthal wire  +/- 1,5°C  air  water  K 
20°C-1250°C  L75/230  kanthal wire  +/- 1,5°C  air  water  S 
20°C-1550°C  L75/240  SiC  +/- 2°C  air  water  S 
20°C-2300°C  L75/260  graphite  +/- 3°C  N2/vacuum  water  pyrometer 
 
Vertical
-150°C-500°C  L75/264  thermo coax  +/- 2°C  air  LN2  K 
20°C-1000°C  L75/220  kanthal wire  +/- 1,5°C  air  water  K 
20°C-1250°C  L75/230  kanthal wire  +/- 1,5°C  air  water  S 
20°C-1550°C  L75/240  SiC  +/- 3°C  air  water  S 
20°C-1750°C  L75/250  pyrox  +/- 3°C  air  water  EL18 
20°C-2300°C  L75/260  graphite  +/- 3°C  N2/vacuum  water  pyrometer 
Horizontal Rule
Mexican Flag
Pagina Principal
 
Introduccion al dilatometro L75 | Dilatometro de levantavalvulas sencillo | Dilatometro de levantavalvulas doble
Sistemas para medir dilatometros | Programas para dilatometros | Aplicaciones para dilatometros
Informacion: info@linseis.com
Webmaster: BRT