Linseis Logo Small

Dilatometer Software


Horizontal Rule

All LINSEIS Thermal Analysis Instruments are controlled through sophisticated Windows® software. The complete program consists of three sections: temperature control, data acquisition, and data evaluation. Essential sample information is entered in the data acquisition section.

Data Acquisition section


Documentation set-up menu

Picture 1: menu for the documentation set-up

Essential data for each sample test includes; operator, laboratory, atmosphere, gas flow, material, sample file name, zero file name, comments, sample length, measuring range, max. temperature, duration of run, sampling frequency, heating and cooling rates, number of cycles.

All menus are easily understood and intuitive. The software is quickly mastered with minimal training needed.


             LINSEIS Dilatometer Evaluation Protocol

Common data:

-----------------------------------------------------------------
Date/Time:  11/14/99  13:38:42  Sample:     Platinum    10.00 mm 
Operator:   Pog                 Reference:  --------     0.00 mm 
Laboratory: LINSEIS             Atmosphere: Air          0.00 l/h
Comment:    Calibration         Zero: Null-10   Piston:  Quartz  
-----------------------------------------------------------------


Controller parameters:

-----------------------------------------------------------------
Segment | Heating  [K/min] |End temperature [°C]| Dwell time[min]
-----------------------------------------------------------------
   1    |       10.0       |       830.0        |        0.0     
   2    |       30.0       |       500.0        |        0.0     
-----------------------------------------------------------------


Table of data and coefficients:

Reference temperature for AKt:  20°C
Reference temperature for AKp:  20°C
-----------------------------------------------------------------
   T [°C]   |   dL [µm]  | AKt[E-6/K] | AKp[E-6/K] |  dL/L0 [%]  
-----------------------------------------------------------------
    100.0   |     6.94   |     8.68   |     9.66   |    0.069    
    200.0   |    16.26   |     9.03   |    10.82   |    0.163    
    300.0   |    25.85   |     9.23   |    11.12   |    0.259    
    400.0   |    35.49   |     9.34   |    11.40   |    0.355    
    500.0   |    45.21   |     9.42   |    11.62   |    0.452    
    600.0   |    55.78   |     9.62   |    11.98   |    0.558    
    700.0   |    66.33   |     9.75   |    12.34   |    0.663    
    800.0   |    77.24   |     9.90   |    12.75   |    0.772    
-----------------------------------------------------------------

Picture 2: results of a print-out

Evaluation section



Evaluation Menu

Picture 3: the evaluation menu

The evaluation is part of the complete windows software, It features a number of functions enabling a full evaluation of all types of data. All evaluation and data collection can be performed simultaneously. Data can be corrected using zero and calibration correction. Data evaluations include: absolute length change, relative length change, and coefficient of thermal expansion. A mean curve with statistical analysis can be performed on multiple curves. Graphical displays can be printed on all windows compatible printers or plotters.

Data can be displayed and printed in a table format. The software also includes an ASCII export feature.


Horizontal Rule

USA Flag
Home

Special Equipment | Dilatometer L75 Introduction | Single Pushrod Dilatometer | Dual Pushrod Dilatometer
Dilatometer Measuring Systems | Dilatometer Furnace Programs | Dilatometer Applications

Information: info@linseis.com
Webmaster: BRT