The measuring system of a dilatometer consists of a sample holder and a push rod. The later one is used to transfer the expansion of the material out of the heated zone to the LVDT. The thermocouple that measures the temperature directly over or in a hole of the sample measures the actual sample temperature. The available measuring systems are as follows:

range material sample TC Type
-150°C - 400°C quartz 7mm K
20°C - 1100°C quartz 14mm K
20°C - 1550°C AI2O3 14mm S
20°C - 1750°C AI2O3 14mm B
20°C - 2300°C graphite 14mm C
Single pushrod sample holder
single pushrod sample holder
Dual pushrod sample holder
dual pushrod sample holder

Horizontal Rule

USA Flag
Home

Special Equipment | Dilatometer L75 Introduction | Single Pushrod Dilatometer | Dual Pushrod Dilatometer
Dilatometer Furnace Programs | Dilatometer Software | Dilatometer Applications

Information: info@linseis.com
Webmaster: BRT