temperature range: -150°C - 500°C temperature range: 20°C - 1000°C temperature range: 20°C - 1250°C
temperature range: 20°C - 1550°C temperature range: 20°C - 1750°C temperature range: 20°C - 2300°C



Horizontal
Temperature Type Element Temp. Variation Atmosphere Coolant TC type
20°C-1000°C L75/220 Kanthal wire +/- 1,5°C air water K
20°C-1250°C L75/230 kanthal wire +/- 1,5°C air water S
20°C-1550°C L75/240 SiC +/- 2°C air water S
20°C-2300°C L75/260 graphite +/- 3°C N2/vacuum water pyrometer

Vertical
-150°C-500°C L75/264 thermo coax +/- 2°C air LN2 K
20°C-1000°C L75/220 kanthal wire +/- 1,5°C air water K
20°C-1250°C L75/230 kanthal wire +/- 1,5°C air water S
20°C-1550°C L75/240 SiC +/- 3°C air water S
20°C-1750°C L75/250 pyrox +/- 3°C air water EL18
20°C-2300°C L75/260 graphite +/- 3°C N2/vacuum water pyrometer

Horizontal Rule

USA Flag
Home

Special Equipment | Dilatometer L75 Introduction | Single Pushrod Dilatometer | Dual Pushrod Dilatometer
Dilatometer Measuring Systems | Dilatometer Software | Dilatometer Applications

Information: info@linseis.com
Webmaster: BRT